ALPHA EF-8000

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

ALPHA EF-8000

Main features

  • Greater Than 96% Hole Fill
  • Low-Bridging Connector Soldering
  • Spray or Foam Application

Product Description

ALPHA EF-8000 Liquid Soldering Flux is a low-rosin, no-clean liquid flux for wave soldering high-density and general circuit-board assemblies across lead-free and tin-lead processes. On bottom-side QFPs and connectors, the formulation targets low bridging while delivering greater than 96% hole-fill yield on 10 mil holes and good micro-solder-ball performance in lead-free applications. Spray or foam application provides process flexibility, and the evenly spread, tack-free residue remains pin-testable. Separate operating ranges are provided for SAC305 and 63Sn37Pb alloys. The liquid typically contains 6.0% solids and has 0.806 specific gravity at 25 deg C, with ROL0 classification.

Key Features

  • High hole-fill yield: Greater than 96% hole-fill yield on 10 mil holes.
  • Low-bridging performance: Designed for low bridging on connectors and bottom-side QFPs.
  • Flexible flux application: Spray or foam application leaves evenly spread, tack-free, pin-testable residue.

Applications

Wave soldering for high-density and general circuit-board assemblies with lead-free or tin-lead alloys using spray or foam application.

Product Family

ALPHA EF-8000

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Solids
6.0 %
Specific Gravity
0.807 ± 0.003 @25°C

Additional Information

Typical Properties

As Supplied

Typical values for the ready-to-use liquid flux.

PropertyTypical ValueUnitsMethod or Condition
AppearanceClear, pale yellow liquidVisual
Solids content6.0% by weightTypical
Specific gravity0.80625 deg C
Acid number27.0mg KOH/gTypical
pH3.15% v/v aqueous solution
Flash point17deg CT.C.C.
Shelf life12monthsTypical
Flux classificationROL0IPC J-STD-004