ALPHA EF-6808HF

Harmonization Code : 3404.90.00.00 | Artificial waxes and prepared waxes : Other

ALPHA EF-6808HF

Main features

  • High-Density Hole-Fill Performance
  • Low-Bridging Wave Soldering
  • Transparent Pin-Testable Residue

Product Description

ALPHA EF-6808HF Liquid Soldering Flux is a ready-to-use, halogen-free, low-solids, alcohol-based no-clean flux for automated and manual circuit-board soldering. It is formulated for single- and dual-wave processes with SnPb and lead-free alloys and is especially effective on assemblies with high-density components. The flux provides strong hole fill with low bridging, icicles, and solder balls, while leaving uniform, transparent, tack-free residues that remain highly pin-testable. Spray application is recommended, with operating ranges for flux loading, preheat, conveyor speed, contact time, and solder-pot temperature. Typical as-supplied data include 4.0% solids, 0.793 +/- 0.005 specific gravity at 25 deg C, and an ROL0 designation.

Key Features

  • High-density hole fill: Excellent hole fill with low bridging on high-density component assemblies.
  • Low-defect wave soldering: Low bridging, icicles, and solder balls in SnPb and lead-free processes.
  • Pin-testable residue: Uniform, transparent, tack-free residue remains highly pin-testable.

Applications

Automated and manual wave soldering with SnPb and lead-free alloys, including high-density component assemblies.

Product Family

ALPHA EF-6808HF

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Solids
4.0 %
Specific Gravity
0.793 ± 0.005 @25°C

Additional Information

Typical Properties

As Supplied

Typical values for the ready-to-use liquid flux.

PropertyTypical ValueUnitsMethod or Condition
AppearanceClear, light amber liquidVisual
Solids content4.0% by weightTypical
Specific gravity0.793 +/- 0.00525 deg C
Acid number19.4 +/- 2mg KOH/gTypical
Flash point17deg CT.C.C.
Shelf life360daysTypical
Flux classificationROL0J-STD-004