ALPHA EF-6100P

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

ALPHA EF-6100P

Main features

  • Broad Lead-Free Process Window
  • Reduced Bridging and Solder Balls
  • Low-Residue Pin-Test Surface

Product Description

ALPHA EF-6100P Liquid Soldering Flux is a low-solids, alcohol-based no-clean flux for wave and selective soldering with lead-free and tin-lead alloys. It is designed for assemblies that require strong through-hole fill, reduced component bridging, and fewer skips. Thermally stable activators support a broad process window, while the formulation resists solder-ball formation across a range of solder masks. Residue is low, non-tacky, and designed to minimize interference with pin testing. Spray application is specified, with separate process ranges for SAC305 or SACX0307 and 63Sn37Pb operation. Typical as-supplied data include 3.8% solids, 0.794 +/- 0.003 specific gravity at 25 deg C, and ORL0 classification.

Key Features

  • Broad soldering window: Thermally stable activators support lead-free and tin-lead wave soldering.
  • Reduced solder defects: Designed for strong through-hole fill with reduced bridging, skips, and solder-ball formation.
  • Pin-testable low residue: Very low, non-tacky residue minimizes interference with pin testing.

Applications

Spray-applied wave and selective soldering for lead-free and tin-lead circuit-board assemblies.

Product Family

ALPHA EF-6100P

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Solids
3.6 %
Specific Gravity
0.794 ± 0.003 @25°C

Additional Information

Typical Properties

As Supplied

Typical values for the ready-to-use liquid flux.

PropertyTypical ValueUnitsMethod or Condition
AppearanceClear, colorless to pale yellow liquidVisual
Solids content3.8% by weightTypical
Specific gravity0.794 +/- 0.00325 deg C
Acid number23.9 +/- 1.2mg KOH/gTypical
pH3.35% aqueous solution
Flash point12deg CT.C.C.
Shelf life360daysFrom date of manufacture
Flux classificationORL0IPC J-STD-004