ALPHA EF-6100-R

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

ALPHA EF-6100-R

Main features

  • Low-solids, alcohol-based no-clean rework flux supporting both lead-free and tin-lead soldering with fast wetting and a wide thermal process window.
  • Very low levels of non-tacky residue help minimize interference with pin testing while supporting no-clean processing.
  • ORL0 classification backed by documented IPC J-STD-004A/J-STD-004B SIR, Bellcore SIR, electromigration, and corrosion test results.

Product Description

ALPHA EF-6100-R No-Clean Rework Flux is a low-solids, alcohol-based flux developed for lead-free and tin-lead rework soldering. Its thermally stable activator and solvent system supports fast wetting across different solder alloys while maintaining a wide thermal process window. The no-clean formulation leaves a very low level of non-tacky residue and is designed to reduce interference with pin testing. ALPHA EF-6100-R is classified ORL0 according to IPC J-STD-004 and has documented surface insulation resistance and electromigration performance. It can be applied using a flux pen, brush, or spray bottle for localized rework operations.

Key features

  • Lead-free and tin-lead rework capability: Provides fast wetting across different Pb-free and SnPb alloys with a wide thermal process window.
  • Low-residue no-clean formulation: Leaves a very low level of non-tacky residue designed to reduce interference with pin testing.
  • Documented electrical reliability: ORL0 flux with documented IPC J-STD-004A/J-STD-004B SIR and Bellcore SIR and electromigration test results.

Applications / Suitable for

  • Lead-free soldering rework
  • Tin-lead soldering rework
  • Localized flux application using flux pens, brushing, or spray bottles
Product Family

ALPHA EF-6100-R

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Solids
4.3 %
Specific Gravity
0.818 ± 0.003 @25°C

Additional Information

Technical properties

As-supplied / before-processing properties

Selected typical properties of ALPHA EF-6100-R in its as-supplied liquid state.

Property Value Unit Method or condition
Appearance Clear, colorless liquid - Typical
Solids content 4.3 % by wt Typical
Acid number 26.2 +/- 1.3 mg KOH/g Typical
Specific gravity 0.818 +/- 0.003 - 25 °C (77 °F)
Flash point 60 (15.6) °F (°C) T.C.C.
pH 3.2 - 5% aqueous solution
Flux classification ORL0 - IPC J-STD-004
Technical properties

After-processing / final-state properties

Selected electrical reliability and corrosion results for uncleaned ALPHA EF-6100-R residues under the stated test conditions.

Property Value Unit Method or condition
SIR - Comb-Down, uncleaned 4.4 x 109 ohms IPC J-STD-004A; 85 °C/85% RH, 7 days, -50 V; measurement at 100 V on IPC B-24 board
SIR - Comb-Up, uncleaned 4.2 x 109 ohms IPC J-STD-004A; 85 °C/85% RH, 7 days, -50 V; measurement at 100 V on IPC B-24 board
SIR - Comb-Down, uncleaned 2.4 x 1012 ohms IPC J-STD-004B TM2.6.3.7; IPC B-24 coupons, 12 V, 40 °C, 90% RH
Bellcore SIR - Comb-Down, uncleaned 4.9 x 1011 ohms GR 78-CORE, Issue 1; 35 °C/85% RH, 4 days, 48 V; measurement at 100 V
Bellcore electromigration - Comb-Down, uncleaned Pass - GR 78-CORE, Issue 1; initial SIR 4.5 x 108 ohms, final SIR 5.2 x 109 ohms; 65 °C/85% RH, 500 hours, 10 V
IPC copper corrosion No evidence of corrosion - ORL0 corrosion testing