ALPHA 856

Harmonization Code : 3404.90.00.00 | Artificial waxes and prepared waxes : Other

ALPHA 856

Main features

  • Neutral Buffered Residue for Water Cleaning
  • Fast-Recovering Foam for Production Coverage
  • Defined Four-Hour Cleaning Window

Product Description

ALPHA 856 Liquid Soldering Flux is a neutral organic-acid, water-soluble liquid flux for wave soldering processes that use post-solder water cleaning. Its buffered activation system contains no free acid, and the post-solder residues are non-acidic. The low-smoking formulation is designed for foam application with a fine-bubble head that breaks quickly and recovers rapidly at production speed. During use, specific gravity at 25 deg C is maintained at 0.822 to 0.842 with ALPHA 425 thinner. Residues remain water soluble and should be thoroughly removed within four hours; hot DI-water rinsing at 50 to 60 deg C is specified for low ionic contamination before drying.

Key features

  • Neutral buffered activation: Contains no free acid and produces non-acidic post-solder residues for controlled water-cleaned soldering processes.
  • Fast-recovering foam coverage: A fine-bubble foam head breaks quickly and recovers rapidly to maintain coverage at production speed.
  • Controlled water-cleaning window: Water-soluble residues should be removed within four hours, with a 50 to 60 deg C hot DI-water rinse used for low ionic contamination.

Applications

Used in water-cleaned wave soldering of electronic assemblies with foam flux application, controlled flux density, and prompt hot DI-water residue removal.

Product Family

ALPHA 856

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Solids
15 %
Specific Gravity
0.832 ± 0.005 @25°C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
AppearanceColorless to pale yellow liquidTypical
Specific gravity0.832 +/- 0.005At 25 deg C (77 deg F)
Non-volatiles15%Typical
pH6.65% solution
Halide as chloride2.33 +/- 0.23%Typical
Flash point17 (62)deg C (deg F)T.C.C.
Shelf life720daysFrom date of manufacture
IPC classificationORH1IPC J-STD-004