ALPHA 3355-HB

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

ALPHA 3355-HB

Main features

  • Broad Conveyor Preheat Window
  • Multi-Method Flux Application
  • Defined Hot-Water Cleaning Process

Product Description

ALPHA LONCO 3355-HB Water Soluble Flux is a clear, water-soluble liquid soldering flux formulated with a surfactant system for a broad preheat window. It is used primarily in foam and conveyorized processes and also supports spray, dip, wave, and brush application. A topside preheat range of 82 to 110 deg C is typical. Monitor specific gravity during use and replace evaporated solvent with ALPHA 3355 Additive. Flux residues must be removed with 50 to 70 deg C water, preferably immediately after soldering and within four hours. Use plastic or titanium for applicators and reservoirs.

Key features

  • Broad preheat window: A typical 82 to 110 deg C topside range gives conveyorized processes practical preheat latitude.
  • Versatile flux application: Foam, spray, dip, wave, and brush methods support multiple soldering-line configurations.
  • Defined residue-removal process: Hot-water cleaning at 50 to 70 deg C within four hours provides a clear post-solder process window.

Applications

Applications include water-soluble fluxing for conveyorized soldering with foam and supported spray, dip, wave, or brush application.

Product Family

ALPHA 3355-HB

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Solids
30 %
Specific Gravity
0.960 ± 0.005 @25°C

Additional Information

Technical properties

As-supplied / before-processing properties

Monitor specific gravity in use and replenish evaporated solvent with ALPHA 3355 Additive.

PropertyValueUnitMethod / condition
AppearanceClear, colorless liquidAs supplied
Solids content30%Typical
Specific gravity0.960 +/- 0.00525 deg C
Flash point71deg FTypical
Acid number40 +/- 4mg KOH/gTypical
Chloride content2.0 +/- 0.2%Typical
Flux classificationORH1IPC J-STD-004
Shelf life540daysFrom date of manufacture