Nanoproof 3-04 is a highly effective electronic coating series designed to provide superior protection against moisture, chemicals, and corrosion for a wide range of electronic applications. With the discontinuation of the popular 3M Novec product line, the Aculon Nanoproof 3.0 series offers a readily available and accessible alternative for industries that require robust protection for their electronic devices.

Nanoproof 3-04 with 4% Fluoroacrylate solids, forms a thin, transparent layer that provides excellent anti-wetting and anti-stiction properties, protecting electronic devices from harmful elements. With this amount of solids, it manages to reach a coating thickness of 0.25 - 2um. The coating also offers electrical insulation properties (3600V/mil Dielectric Strength), reducing the risk of electrical shorts and failures of PCBs and Electrical components.

The Aculon Nanoproof 3.0 series comes in different grades, with Aculon Nanoproof 3-04 offering similar performance and chemical properties to the 3M Novec 1904 and 2704 products. It is ideal for use in harsh environments, making it a popular choice in industries such as automotive, aerospace, and defense. Aculon Nanoproof 3-04 is easy to apply, and its transparent coating ensures that it does not interfere with the aesthetics or functionality of electronic devices. It is suitable for use on a variety of electronic applications, including printed circuit boards, sensors, switches, and connectors.

Product Family

ACULON NanoProof 3-04

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 6 weeks
CA Shipping in 6 weeks
EU Shipping in 6 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Light Green
Refractive index
1.376
Solids
Fluoroacrylate 4 %
Thermal Properties
Glass Transition Temperature (Tg)
95 °C
Electrical Properties
Dielectric Strength
3600 kV/mm
Other Properties
Oil Contact Angle
80 °
Water Contact Angle
120 °
Physical Properties
Viscosity
20 mPa.s

Additional Information

Thickness depends on the amount of Solids. The higher the amount of solids, the thicker the coating after the solvent evaporates.

 

Aculon Nanoproof 3-04 vs 3M Novec 1904 and 2704

  3M Novec 1904 3M Novec 2704 Aculon Nanoproof 3-04
Solids Fluoroacrylate 4% Fluoroacrylate 4% Fluoroacrylate 4%
Solvent 7100/7200 7200 + 5% PGMEA 347
Appearance Clear Yellow - Orange Light Green
Density 1.43 g/ml 1.4 g/ml 1.5 g/ml
Viscosity 1.11 cP 1.75 cP <20 cP
Boiling point 75°C 78°C 56°C
Environmental Non ozone depleting, low in toxocity, low in GWP, RoHS compliant and VOC exempt per US-EPA, contains no chlorine or bromine Non ozone depleting, low in toxocity, low in GWP, RoHS compliant and VOC exempt per US-EPA, contains no chlorine or bromine Non ozone depleting, low in toxocity, low in GWP, RoHS compliant and VOC exempt per US-EPA, contains no chlorine or bromine
Shelf life 2 years 2 years 2 years
Thickness 0.5 - 6um 0.1 - 4um 0.25 - 2um
Tg 44.5°C 53°C 95°C
Thermal Stability of dry film Can withstand 175°C for 24h and maintain repellency Can withstand 175°C for 24h and maintain repellency Can withstand 175°C for 24h and maintain repellency
Contact angles WCA/OCA: 105°/65° WCA/OCA: 105°/65° WCA/OCA: 120°/80°
Refractive Index 1.39 1.39 1.376
Solder through repairability Yes Yes Yes
Non-flammability Meets UL 94 V-0 Meets UL 94 V-0 Will meet UL 94 V-0 (Met via 5.5)
Dielectric Strength @ 35% RH 2000 V/mil 2500 V/mil 3600 V/mil
Cure None None None
Application Anti stiction, Chemical protection, Corrosion protection, Moisture protection Anti stiction, Chemical protection, Corrosion protection, Moisture protection Anti stiction, Chemical protection, Corrosion protection, Moisture protection
Application location PCB, Electrical components PCB, Electrical components PCB, Electrical components