Aculon 73DE Offset
Harmonization Code : 2901.10.00.00 | Acyclic hydrocarbons; Saturated
Main features
- Fluorinated Solvent
- Heavy duty vapor degrease
- 3M Novec 73DE alternative
Product Description
Aculon 73DE Offset is a clear fluorinated solvent blend designed for heavy-duty vapor degreasing or immersion cleaning applications. Some of the features include high solvency, low surface tension, non-flammability, and fluid stability.
Vapor degreasing with Aculon 73DE fluid can help save time and costs over by offering faster cycle times, lower energy usage, and improved cleaning of parts with complex geometries. It is a direct replacement for Novec 73DE.
Key Features
- Effective in cleaning heavy greases, oils, waxes, silicones, and non-polar flux residues.
- Easy maintenance and use in a vapor degreaser with stable bath composition during extended use.
- Non-flammable and low in toxicity.
- Environmentally sustainable with low global warming potential (GWP) and 0 ozone depletion potential(ODP).
- Replacement for Novec 73DE, nPB, TCE, ozone-depleting HCFCs, and high GWP HFCs.
- Effective for lubricant deposition applications where increased solvency is desired.
Packaging
Please select Package Type.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Appearance
clear/colorless
Solids
none %
Specific Gravity
1.28
Vapor Pressure
0.36 kg/cm2
Thermal Properties
Boiling Point
48 °C
Physical Properties
Viscosity
1 mPa.s
Additional Information
Aculon 73DE Offset vs 3M Novec 73DE
| 3M Novec 73DE | Aculon 73DE | |
| Viscosity (cP) | 0.38 cP | <1 cP |
| Liquid Density (g/mL) | 1.28 | 1.28 |
| Boiling point (°C) | 48 | 48 |
| Surface Tension (dynes/cm) | 19.9 | 19.9 |
| Kauri-Butanol Value | 83 | 83 |
| Vapor Pressure (mm/Hg @ 20 °C) | 263 | 263 |
| Heat of Vaporization (cal/g @ boiling point) |
54.2 | 54.2 |
| Shelf life | 2 years | 2 years |
Aerospace Materials Compatibility
| Test Description | ASTM Method | Test result |
| Sandwich Corrosion | F1110 | Passes |
| Effect on Painted Surfaces | F502 | Passes |
| Hydrogen Embrittlement | F519 | Passes |
| Effect on Unpainted Surfaces | F485 | Passes |
| Total Immersion Corrosion | F483 | Passes |
| Low-Embrittling Cadmium Plate | F1111 | Passes |
| Flash Point | D56 | Passes |
| Acrylic Stress Crazing | F484 | Does Not Pass |
| Stress Corrosion of Titanium Alloys | F945 | Passes |
Compatibility with Materials
| Plastics | Compatible | Acetal, Epoxy, Nylon, PEEK, Polyester, Polyethylene, Polypropylene, PTFE |
| Plastics | Incompatible | ABS, Polystyrene, Acrylic, Polycarbonate |
| Elastomers | Compatible | DuPont Kalrez Perfluoroelastomers, Butyl Rubber, Parfluor Perfluoroelastomers, Viton Fluoroelastomers, Polyurethane |
| Elastomers | Incompatible | Silicone, Fluorosilicone |
| Metals | Compatible | Copper, Brass, Stainless Steel, Magnesium, Titanium, Aluminum, Carbon Steel, Cadmium |
| Metals | Incompatible | No Data |