LOCTITE ABLESTIK TE3530

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE ABLESTIK TE3530

Main features

  • One component
  • Thermally conductive
  • Low viscosity

Product Description

LOCTITE ABLESTIK TE 3530 adhesive is designed for bonding heat dissipation components and can be applied by automatic syringe dispense. It cures at moderate to low temperatures allowing it to be used on heat sensitive materials.

LOCTITE ABLESTIK TE 3530 is a white, thermally conductive epoxy adhesive with low temperature cure that is typically used in sensor and die attach assemblies. Operating temperature is 150°C.

Cure Schedule

  • 30 minutes @ 100°C or
  • 15 minutes @ 120°C or
  • 10 minutes @ 150°C
Product Family

ABLESTIK TE3530

1. Select Package Type
2. Select Package Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 37 days
CA Shipping in 12 weeks
EU Shipping in 25 days
Packaging
Please select Package Type and Package Size.
TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Thermal Conductivity
2.3 W/m.K
Physical Properties
Viscosity
60,000 mPa.s