LOCTITE ABLESTIK QMI9507-2C2

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE ABLESTIK QMI9507-2C2

Main features

  • Controlled bondline thickness
  • High thermal conductivity
  • Stable at high temperatures

Product Description

LOCTITE ABLESTIK QMI9507-2C2 is developed as a soft solder alternative for applications requiring high thermal or high electrical conductivity. It contains spacers for improved bondline control. The optimized loading percentage is such that other bulk properties of the material remain unaffected. This product and its use may be covered by patent 5,716,034 and by one or more pending patent applications.

LOCTITE ABLESTIK QMI9507-2C2 has a proprietary hybrid chemistry that can be heat cured or snap cured. It's spacer size is ~50um and is typically used for the attachment of intergrated circuits and components to metallic leadframes. It can be used on a wide variety of substrates such as metals, Ceramic surfaces, Copper, Ni/Pd/Au, Alloy 42 leadframes and Silver-plated copper leadframes.

LOCTITE ABLESTIK QMI9507-2C2 is designed to achieve UPHs several orders of magnitude higher than conventional oven cured adhesives. Maximum productivity is realized through in-line cure, either on the diebonder using a post diebond heater or on the wirebonder preheater.

 

Oven Cure

  • 30 minutes @ 185°C

Snap Cure

  • 7-Zone Oven:
  • Temp per zone: 170ºC, 170ºC, 170ºC, 190ºC, 190ºC, 190ºC, 190ºC
  • Time per zone, seconds 10
Product Family

ABLESTIK QMI9507-2C2

No longer available

This product is no longer available from Krayden. Please contact us so we can recommend an alternative product.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific Gravity
4.10
Work life @25°C
24 hours
Thermal Properties
Glass Transition Temperature (Tg)
3.3 °C
Thermal Conductivity
6.5 W/m.K
Physical Properties
Thixotropic index
4.8
Viscosity
18,500 mPa.s