LOCTITE ABLESTIK QMI534

Main features

  • Hydrophobic
  • Void free bondline
  • Excellent interfacial adhesion strength

Product Description

LOCTITE® ABLESTIK QMI534 is a Fluoropolymer filled non-conductive adhesive for attachment of integrated circuits and components to advanced substrates, including PBGAs, CSPs, array packages, and stacked die.

LOCTITE® ABLESTIK QMI534 is a white, Bismaleimide resin based, hydrophobic product that is stable and adheres best after repeated exposure at high temperatures. It exhibits excellent interfacial adhesion and is mainly used for semiconductor and non conductive adhesive applications.

Cure Schedule

  • ≥6 seconds @ 240°C (SkipCure)
  • 15 minutes @ 150°C (Conventional Oven)
Product Family

ABLESTIK QMI534

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Pot Life
24 hours
Specific Gravity
1.25
Thermal Properties
Glass Transition Temperature (Tg)
-35 °C
Thermal Conductivity
0.4 W/m.K
Chemical Properties
Moisture absorption
0.35 %
Physical Properties
Thixotropic index
5.0
Viscosity
9,000 mPa.s