LOCTITE ABLESTIK NCA 2286

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE ABLESTIK NCA 2286

Main features

  • Dual Cure
  • High elongation strength
  • Active alignment in lens holder attach

Product Description

LOCTITE ABLESTIK NCA 2286 dual cure  acrylic adhesive is designed for use in active alignment applications in camera module assembly. It has been formulated to a high viscosity and thixotropy to enable higher aspect ratios of dispensed adhesive, thus allowing for easier adjustments for the final assembly. This material jas a very high dispense aspect ration and is engineered to meet the high reliability performance requirements for the optoelectronic / semiconductor industry.

LOCTITE ABLESTIK NCA 2286 is black in color to prevent light penetration into the final assembled device. It is designed to achieve fast cure response at low temperatures and good depth of cure after UV radiation. This product also contains a secondary thermal cure mechanism for applications with shadowed areas where light is unable to penetrate. It is a camera/sensor market material that is not expected to pass very harsh reliability requirements.

Cure Schedule
UV Light

  • UV Wavelength, nm 220 to 380
  • Light Intensity, mW/cm² 1,000
  • Exposure Time, seconds 4

Secondary Heat Cure

  • 1 hour @ 80°C
Product Family

ABLESTIK NCA2286

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 60 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Glass Transition Temperature (Tg)
28 °C
Mechanical Properties
Elongation
60 %
Physical Properties
Thixotropic index
5.7
Viscosity
40,000 mPa.s

Additional Information

LOCTITE ABLESTIK NCA 2286 epoxy acrylate has, proven, good adhesion on glass and metals (see test data on 3x3mm glass die on difficult to bond nickel substrate below)