Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Loctite Ablestik JM7000

Main features

  • Low moisture in cavity
  • Low ionic impurities
  • Minimal voiding

Product Description

LOCTITE ABLESTIK JM 7000 die attach adhesive has been formulated for use in high throughput die attach applications and hermetic packages. This material has been used successfully on rigid substrates with die sizes up to 700 mils. LOCTITE ABLESTIK JM 7000 is very stable in high temperatures and has been approved by DESC and Rome Laboratory for military products.

LOCTITE ABLESTIK  JM7000 is a cyanate ester, solvent-containing formulation so it will behave similarly to other Cyanate ester products.The degradation temperature, otherwise known as Onset decomposition temperature provided by the TGA for almost identical products shows decomposition of 0.3% at 400°C so JM7000 should be affected in a similar manner.

Typical Cure Schedule

  • 30 min @ 150°C 

For applications that require higher electrical conductivity, a cure cycle of 15min @ 300°C is recommended.

Product Family

ABLESTIK JM7000

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 21 days
CA Shipping in 12 weeks
EU Shipping in 45 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Work life @25°C
16 hours
Thermal Properties
Glass Transition Temperature (Tg)
240 °C
Thermal Conductivity
1.1 W/m.K
Physical Properties
Viscosity
9,000 mPa.s

Additional Information

 

 

These products are old and so is the data accompanying them. Here is a TGA scan on an already cured JM7000 sample that shows that as the temperature increases the polymer starts to break down. Adhesion strength will start to decrease as the temperature increases approximately past 300°C and it's possible that this weight loss is indication of outgassing or decomposition. Please check the Technical documents section for a new(er) and full(er) data package.