ABLESTIK GA 47-2LV

Harmonization Code : 5906100000 | Adhesive tape of a width not exceeding 20cm

ABLESTIK GA 47-2LV

Main features

  • Gyro-Flotation-Fluid-Compatible Instrument Bonding
  • 25 ppm/deg C Linear Thermal Expansion
  • 2-Hour 95 deg C Cure

Product Description

LOCTITE® ABLESTIK GA 47-2LV is a green, low-viscosity, heat-cured epoxy instrument adhesive. It is documented as compatible with conventional gyro flotation fluids and has a coefficient of thermal expansion that approximates aluminum within a normal temperature range. The material provides a typical viscosity of 50,000 mPa·s, a 30-minute work life at 25°C, and guideline cure options of 2 hours at 95°C or 4 hours at 75°C. Cured aluminum-to-aluminum lap shear strength is reported as 13.8 N/mm². :contentReference[oaicite:0]{index=0}

Key features

  • Gyro-fluid compatibility: Documented compatibility with conventional gyro flotation fluids supports evaluation for applicable instrument assemblies. :contentReference[oaicite:1]{index=1}
  • Aluminum-matched thermal expansion: The coefficient of thermal expansion approximates that of aluminum within a normal temperature range. :contentReference[oaicite:2]{index=2}
  • Heat-cure flexibility: Guideline cure schedules include 2 hours at 95°C or 4 hours at 75°C. :contentReference[oaicite:3]{index=3}

Applications / Suitable for

  • Instrument bonding applications
  • Assemblies involving conventional gyro flotation fluids
  • Bonding aluminum components under the documented cure conditions
Product Family

ABLESTIK GA 47-2LV

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Green
Chemistry Type
Epoxy
Specific Gravity
2.1
Work life @25°C
0.5 hours
Thermal Properties
Glass Transition Temperature (Tg)
95 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties and processing characteristics of the adhesive before cure. :contentReference[oaicite:4]{index=4}

Property Value Unit Method / condition
Technology Epoxy — As supplied
Appearance Green liquid or paste — TDS appearance and SDS physical state
Viscosity 50,000 mPa·s (cP) Test method and temperature not stated
Specific gravity 2.1 — As supplied
Work life 30 minutes At 25°C
Shelf life 365 days At -40°C
Cure schedule 2 hours or 4 hours — 2 hours at 95°C or 4 hours at 75°C; guideline recommendations
Technical properties

After-processing / final-state properties

Typical properties and performance data for the cured adhesive. Values are reference data rather than product specifications. :contentReference[oaicite:5]{index=5}

Property Value Unit Method / condition
Hardness 90 Shore D Test method and cure condition not stated
Glass-transition temperature 95.0 °C Method and cure condition not stated
Coefficient of linear thermal expansion — below Tg 25 ppm/°C Below Tg; method and cure condition not stated
Lap shear strength — aluminum to aluminum 13.8 (2,000) N/mm² (psi) Substrate preparation, bondline, cure condition, test method, and test temperature not stated