LOCTITE ABLESTIK G500

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

LOCTITE ABLESTIK G500

Main features

  • One component
  • General purpose
  • Sag resistant

Product Description

LOCTITE ABLESTIK G 500 is a low viscosity, general purpose epoxy adhesive and sealant that cures to a high gloss finish.

LOCTITE ABLESTIK G 500 is non abrasive with excellent dielectric properties and resistance to heat and water. This heat curable adhesive is typically used for the insulation of copper and other materials and to attach leads to coils. It binds well on copper, rigid plastics and other metals.

 

Cure Schedule

  • 60 minutes @ 125°C or
  • 20 minutes @ 150°C or
  • 5 minutes @ 175°C

 

Product Family

ABLESTIK G500

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 57 days
CA Shipping in 12 weeks
EU Shipping in 50 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Density
1450 kg/m3
Electrical Properties
Dielectric Strength
15 kV/mm
Volume Resistivity
200000000000000 Ohms⋅cm