LOCTITE ABLESTIK ECF 564AHF

Harmonization Code : 3920.99.28.90 | Other plates, sheets, film, foil and strip, of plastics, non-cellular and not reinforced, laminated, supported or similarly combined with other materials ; Of other plastics ; Other; Other

LOCTITE ABLESTIK ECF 564AHF

Main features

  • High flow version of 564A
  • Excellent thermal conductivity
  • Passes Mil 5011 and NASA outgassing

Product Description

LOCTITE ABLESTIK ECF 564AHF adhesive film is designed for use in hybrid packages where outgassing and ionic contamination must be kept to a minimum. This isotropically electrically conductive adhesive film has excellent thermal conductivity and comes with a glass fabric carrier.

LOCTITE ABLESTIK ECF 564AHF is the High flow version of ECF 564A and meets the NASA outgassing requirements and those of MIL-STD883C, Method 5011

 

Cure Schedule

  • 2 hours @ 150°C
Product Family

ABLESTIK ECF564AHF

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 26 days
CA Shipping in 12 weeks
EU Shipping in 50 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Glass Transition Temperature (Tg)
122 °C
Thermal Conductivity
3 W/m.K
Weight Loss @ 300°C
0.15 %
Electrical Properties
Volume Resistivity
0.0004 Ohms⋅cm