LOCTITE ABLESTIK ECF 564A is a configurable silver-filled epoxy film with a glass-fabric carrier for electrically conductive hybrid-package assembly. It is supplied as sheet stock or die-cut preforms, with thickness and dimensions selected for the supplied configuration. It has a 3-day work life at 25 deg C and a recommended cure of 2 hours at 150 deg C. The cured film has a typical volume resistivity of 0.0004 ohm cm and joint resistance of 0.002 ohm per 0.5 in^2 through gold joints. The product meets MIL-STD-883C, Method 5011, and is available only with 5011 certification.

Key features

  • Glass-reinforced conductive film: A silver-filled epoxy coating on glass fabric provides a preformed conductive bonding layer for package assembly.
  • Low-outgassing package assembly: NASA outgassing values and controlled ionic data support hybrid packages that require low contamination.
  • Method 5011 compliance: The product meets MIL-STD-883C, Method 5011, and is supplied only with 5011 certification.

Applications

Applications include hybrid-package assembly and electrically conductive film bonding in supported package constructions.

Product Family

ABLESTIK ECF564A-1

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Silver
Work life @25°C
72 hours
Thermal Properties
Glass Transition Temperature (Tg)
150 °C
Electrical Properties
Volume Resistivity
0.0004 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Supplied thickness and dimensions depend on the selected sheet or die-cut configuration.

PropertyValueUnitMethod / condition
AppearanceSilver filmAs supplied
ConstructionSilver-filled epoxy on glass fabricAs supplied
Work life3days25 deg C
Shelf life365days-40 deg C; from date of manufacture
Available formsSheet stock or die-cut preformsDimensions are configuration-specific
Cure schedule2hours150 deg C; guideline recommendation
Technical properties

After-processing / final-state properties

Final-state values are typical for cured ECF 564A material and the stated joint configurations.

PropertyValueUnitMethod / condition
Coefficient of thermal expansion, below Tg30ppm/deg CTMA
Glass transition temperature150deg CTMA
Thermal conductivity2.2BTU ft^-1 h^-1 deg F^-1121 deg C
Volume resistivity0.0004ohm cmTypical cured film
Joint resistance0.002ohm per 0.5 in^2Measured through gold joints
Lap shear strength2,200psiAluminum-to-aluminum; 25 deg C
Lap shear strength1,800psiGold-to-gold; 25 deg C
NASA outgassingTML 0.3; CVCM <0.01; WVR 0.18%Typical cured material