ABLESTIK D275

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

ABLESTIK D275

Main features

  • 31 N/mm^2 Aluminum Lap Shear
  • 60-Minute 100 deg C Cure
  • Semi-Rigid Cured Material

Product Description

LOCTITE® ABLESTIK D 275 is a one-component, heat-cured epoxy adhesive for high-strength structural bonding of metals, plastics, and ceramics. The black liquid cures to a semi-rigid material intended to reduce stress on bonded components while providing good toughness. Typical cured performance includes aluminum-to-aluminum tensile lap shear strength of 31 N/mm² at 25°C and tensile peel strength of 2,100 N/m. Guideline cure schedules range from 60 minutes at 100°C to 6 minutes at 160°C, with a documented operating-temperature range of -40 to 130°C.

Key features

  • High structural-bond strength: Typical aluminum-to-aluminum tensile lap shear strength is 31 N/mm² at 25°C.
  • Fast heat-cure options: Guideline schedules include 60 minutes at 100°C, 20 minutes at 120°C, or 6 minutes at 160°C.
  • Semi-rigid cured material: Designed to reduce stress on bonded components while maintaining good toughness and peel strength.

Applications / Suitable for

  • High-strength structural bonding
  • Bonding metals
  • Bonding plastics
  • Bonding ceramics
Product Family

ABLESTIK D275

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Black liquid
Chemistry Type
Epoxy
Density (g)
1.14 g/cm3
Thermal Properties
Operating Temperature
-40 to 130 °C
Physical Properties
Viscosity
70000 mPa.s
Chemical Properties
Water Absorption
0.8 %
Electrical Properties
Volume Resistivity
6.0×10¹⁴ Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties, storage information, and guideline cure schedules for the adhesive before final processing.

Property Value Unit Method / condition
Technology Epoxy — One-component adhesive
Appearance Black liquid — As supplied
Density 1.14 g/cm³ ASTM D792
Brookfield viscosity 70,000 mPa·s (cP) ASTM D2393; spindle 6, 5 rpm
Shelf life 122 days At 25°C
Cure schedule 60 minutes, 20 minutes, or 6 minutes — 60 minutes at 100°C, 20 minutes at 120°C, or 6 minutes at 160°C; guideline recommendations
Technical properties

After-processing / final-state properties

Typical cured-material properties and bonded-joint performance. Values are reference data and are not product specifications.

Property Value Unit Method / condition
Operating-temperature range -40 to 130 °C Documented product range
Hardness at 25°C 80 Shore D ASTM D2240
Hardness at 120°C 75 Shore A ASTM D2240
Water absorption 0.8 % ASTM D570
Volume resistivity at 25°C 6.0 × 1014 ohm-cm ASTM D257
Tensile lap shear strength — aluminum to aluminum 31 (4,500) N/mm² (psi) ASTM D1002; tested at 25°C
Tensile peel strength — aluminum to aluminum 2,100 N/m ASTM D1876; tested at 25°C