LOCTITE ABLESTIK CE3520-3

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE ABLESTIK CE3520-3

Main features

  • Nickel filled
  • For mismatched CTE
  • Basic conductivity

Product Description

LOCTITE ABLESTIK CE 3520-3 is a nickel-filled epoxy adhesive that combines a high elasticity with good adhesion on a variety of surfaces, making it suitable for applications with mismatched CTE.

LOCTITE ABLESTIK CE 3520-3 is a low-stress, flexible epoxy that is typically used for component attach and heat sink bonding. The nickel filler lends to the product some basic electrical conductivity. This material can operate in temperatures between -45 to 125°C

Cure Schedule

  • 60 minutes @ 120°C or
  • 30 minutes @ 150°C

 

Product Family

ABLESTIK CE3520-3

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 38 days
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

Electrical Properties
Volume Resistivity
0.2 Ohms⋅cm
Physical Properties
Viscosity
73,000 mPa.s