LOCTITE ABLESTIK CE3103WLV

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Loctite Ablestik CE3103WLV

Main features

  • Pb Free alternative to solder
  • Compatible with non noble metals
  • Optimized for dispensing

Product Description

LOCTITE® ABLESTIK CE 3103WLV is a rigid, Ag filled, one component electrically conductive epoxy adhesive that is a Lead free / Pb-free alternative to solder. It is compatible with non-noble metals and curable under standard solder reflow profiles.

LOCTITE® ABLESTIK CE 3103WLV can be cured using standard solder reflow profiles. Its low viscosity and anti corrosion technology makes it ideal for dispensing. Its operating temperature is -40 up to 150°C.

LOCTITE® ABLESTIK CE 3103WLV passes NASA outgassing standards and it can be used to bond Sn finished passives and components. Common applications include and are not limited to:

  • Bonding of noble passive components onto noble terminated LTCC boards
  • Bonding of Sn or AgSn coated Cu ribbon to front contact (TCO) of thin film PV cells

Cure Schedule

  • 10min @ 120°C or
  • 3min @ 150°C

Technical Specifications

Thermal Properties
Glass Transition Temperature (Tg)
114 °C
Thermal Conductivity
1.8 W/m.K
Electrical Properties
Volume Resistivity
0.0008 Ohms⋅cm
Physical Properties
Thixotropic index
5.5
Viscosity
20,000 mPa.s

Additional Information

Adhesion Strength Comparison (2x2mm Si Die on Au and SS substrate)

Leading Brands Trust in Our Products and Services