ABLESTIK CE 3511PHV

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

ABLESTIK CE 3511PHV

Main features

  • Extended Dispensing Pot Life
  • No-Bleed Conductive Placement
  • Fast Hot-Plate Cure Option

Product Description

LOCTITE ABLESTIK CE 3511PHV is a one-part, silver-filled, electrically conductive epoxy adhesive for circuit assembly. The silver paste is designed for dispensing, has no bleed, and provides a pot life greater than 14 days at 18 to 25 deg C. Heat-cure options range from 60 minutes at 100 deg C to a hot-plate cure of 60 seconds or less at 180 to 190 deg C, although lower-temperature curing reduces electrical conductivity. After cure at 180 deg C, the typical volume resistivity is 5 x 10^-4 ohm cm. The cured adhesive has a typical glass transition temperature of 100 deg C and tensile lap shear strength of 12 N/mm^2.

Key features

  • Long dispensing window: A pot life greater than 14 days at 18 to 25 deg C supports extended dispensing operations.
  • No-bleed silver paste: The one-part paste is designed for dispensing and limits resin bleed during component placement.
  • Flexible heat-cure schedule: Multiple oven and hot-plate options balance cure time and temperature, with lower-temperature cure reducing conductivity.

Applications

Applications include circuit assembly, die attach, component bonding, and attachment of heat-sensitive components.

Product Family

ABLESTIK CE 3511PHV

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Silver
Component System
One
Pot Life
>14 days
Thermal Properties
Operating Temperature
150 °C
Physical Properties
Viscosity
62,500 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Lower-temperature curing reduces the resulting electrical conductivity.

PropertyValueUnitMethod / condition
AppearanceSilver pasteAs supplied
Filler typeSilverAs supplied
Viscosity62,500mPa sBrookfield TD; 10 rpm
Pot life>14days18 to 25 deg C
Shelf life182days-25 to -18 deg C
Cure schedule60 at 100; 45 at 120; 20 at 150; <=1 at 180 to 190minutes at deg CGuideline oven or hot-plate cure options
Technical properties

After-processing / final-state properties

Values are typical for cured LOCTITE ABLESTIK CE 3511PHV under the stated conditions.

PropertyValueUnitMethod / condition
Operating temperature150deg CProduct operating limit
Glass transition temperature100deg CTypical cured material
Coefficient of linear thermal expansion124ppm/deg CTypical cured material
Volume resistivity5 x 10^-4ohm cmCured at 180 deg C
Tensile lap shear strength12N/mm^2Typical cured material

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers