LOCTITE ABLESTIK CDF 625P

Harmonization Code : 7115.90.00.00 | Other articles of precious metal or of metal clad with precious metal : Other

LOCTITE ABLESTIK CDF 625 LOCTITE ABLESTIK CDF 625 LOCTITE ABLESTIK CDF 625

Main features

  • Electrically conductive
  • Thermally conductive
  • Low warpage

Product Description

LOCTITE® ABLESTIK CDF 625P silver filled, die attach adhesive film is the most universal film, compatible with pre-cut wafer lamination equipment, recommended for large die applications. It is suitable for bonding integrated circuits and components with low warpage and good adhesion (>5MPA) on laminates and metal finishes. Furthermore, it has the lowest total cost of ownership and covers a wide die size range up to 10x10mm.

LOCTITE® ABLESTIK CDF 625P has a broad application space with controlled 25um bondline and a low modulus that is very close to Ablestik 8322A (2000 MPa @ RT, 40 MPa @ 250C.). This conductive die attach film can be effectively used for other applications and can also be a potentially replacement for QMI519.

Cure Schedule

  • 30 minute ramp to 100°C + 30 minutes @ 100°C +
  • 30 minute ramp to 175°C + 1 hour @ 175°C
Product Family

ABLESTIK CDF625P

1. Select Package Type
2. Select Pieces per roll
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 20 days
CA Shipping in 8 weeks
EU Shipping in 45 days
Packaging
Please select Package Type and Pieces per roll.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Work life @25°C
1440 hours
Thermal Properties
Glass Transition Temperature (Tg)
-5 °C
Thermal Conductivity
1 W/m.K
Electrical Properties
Volume Resistivity
0.008 Ohms⋅cm

Additional Information

How is CDF 625P packaged and "rolled?


Henkel has worked with its suppliers to improve the Conductive Die Attach Film (cDAF) product line by developing an edge tape layer to mitigate the occurrence of impression marks.
Two “Edge Tapes” are applied acting like a shim to reduce the contact pressure on the adhesive circles and potential impression marks on the roll. As these 2 “Edge Tapes” are applied outside of the functional CDF 625P adhesive circle, there’s no impact on Fit, Form, or Function! This makes this a major improvement without any effect to your current process.
 
 

CDF 600P - Die attach film property comparison

 