LOCTITE ABLESTIK ABP 8068TI

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE ABLESTIK ABP 8068TI

Main features

  • High thermal and electrical properties
  • Low sintering temperature
  • High reliability

Product Description

LOCTITE ABLESTIK ABP 8068TI is a silver-filled, pressure less die attach adhesive designed for semiconductor packages with high thermal and electrical requirements. This material’s epoxy assisted sintering formulation is designed to provide high adhesion, high thermal and low stress properties which are essential for thermal and reliability performances of high end power packages. ABLESTIK ABP 8068TI has shown a better thermal performance compared to a solder paste material.

LOCTITE ABLESTIK ABP 8068TI is the enhanced sintering performance version of LOCTITE ABLESTIK ABP 8068TA adhesive with similar workability.

Product Family

ABLESTIK ABP8068TI

1. Select Package Type
2. Select Package Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 35 days
Packaging
Please select Package Type and Package Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Work life @25°C
24 hours
Thermal Properties
Thermal Conductivity
165 W/m.K
Weight Loss @ 300°C
-4 %
Electrical Properties
Volume Resistivity
0.000009 Ohms⋅cm
Physical Properties
Thixotropic index
6.5
Viscosity
13000 mPa.s

Additional Information

Recommended Cure Schedule

  • For the die size <5 x 5 mm:
    • 20 minutes ramp from 25°C to 130°C, hold for 30 to 60 minutes; 15 minutes ramp to 200°C, hold for 60 minutes in air or N2 oven 
  • For the die size >5 x 5 mm:
    • 20 minutes ramp from 25°C to 130°C, hold for 120 minutes; 15 minutes ramp to 200°C, hold for 60 minutes in air or N2 oven
  •  Alternate Cure Schedule (suitable for Ag, Au and PPF substrates)
    • 20 minutes ramp from 25°C to 130°C, hold for 30 to 60 minutes; 10 minutes ramp to 175°C, hold for 60 minutes in N2 or air oven

Thawing

  1. Allow container to reach room temperature before use.
  2. After removing from the freezer, set the syringes to stand vertically while thawing.
  3. Refer to the Syringe Thaw time chart for the thaw time recommendation.
  4. DO NOT open the container before contents reach 25°C temperature. Any moisture that collects on the thawed container should be removed prior to opening the container.
  5. DO NOT re-freeze. Once thawed to 25°C, the adhesive should not be re-frozen

Thawing graph of LOCTITE ABLESTIK ABP 8068TI

Directions for Use

  1. Thawed material should immediately be placed on dispense equipment for use.
  2. If the adhesive is transferred to a final dispensing reservoir, care must be exercised to avoid entrapment of contaminants and/or air into the adhesive.
  3. Adhesive must be completely used within the product's recommended work life.
  4. Bondline thickness guideline:
    • Die Size <=3 x 3 mm², BLT control, µm: 10 to 25
    • Die Size >3 x 3 mm², BLT control, µm: 20 to 50

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers