LOCTITE ABLESTIK ABP 8060T

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE ABLESTIK ABP 8060T

Main features

  • High heat transfer
  • Soft solder replacement
  • Stable at high temperatures

Product Description

LOCTITE® ABLESTIK ABP 8060T is formulated to provide high heat transfer generated from power devices. This material can also be used as a soft solder alternate for applications requiring very high thermal and electrical conductivity.

LOCTITE® ABLESTIK ABP 8060T is a hydrophobic, electrically and thermally conductive BMI hybrid that is stable at high temperatures. This silver paste it typically used for MOSFET packages and exhibits high die shear strength.

Cure Schedule

  • 45 minutes ramp from 25°C to 200°C + 60 minutes @ 200°C in N2 or air oven
  • 30 minutes ramp from 25°C to 175°C + 60 minutes @ 175°C in N2 or air oven
Product Family

ABLESTIK ABP8060T

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 35 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Filler Content
85 %
Work life @25°C
24 hours
Thermal Properties
Thermal Conductivity
20 W/m.K
Electrical Properties
Volume Resistivity
0.000025 Ohms⋅cm
Physical Properties
Thixotropic index
6
Viscosity
12,000 mPa.s

Additional Information

It's stated in the TDS that it needs a N2 oven. Is this a prerequisite? Can it be cured in a conventional oven and if so how will this change the cure schedule?

Many customers prefer to cure in Nitrogen, to protect components from oxidation. But curing both in Air or Nitrogen is still OK. Die shear strength is not significantly affected by the curing atmosphere.