LOCTITE ABLESTIK ABP 8037TI

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Loctite Ablestik ABP8037TI

Main features

  • High-reliability LED manufacture
  • High thermal conductivity
  • Small die on Au-finish LF

Product Description

LOCTITE ABLESTIK ABP 8037TI silver-filled conductive adhesive is recommended for use in the attachment of integrated circuits and components onto metal leadframes and advanced substrates.

LOCTITE ABLESTIK ABP 8037TI silver-filled die attach adhesive paste is specifically designed to attach small diodes in high volume manufacturing. Even more specifically, it is the highest volume silver-filled die attach paste for high reliability LED attach and manufacture when using small die on Au-finished leadframes. Used in high-volume manufacturing throughout China and Malaysia.

LOCTITE ABLESTIK ABP 8037TI is similar to Loctite Ablestik ABP 8037T, with a minor raw material change that made it adjust its naming convention.

Cure Schedule

  • 30 minute ramp to 175ºC, hold 30 minutes @ 175 °C
  • 30 minute ramp to 150ºC, hold 30 minutes @ 150 °C

 

 

Product Family

ABLESTIK ABP8037TI

1. Select Package Type
2. Select Package Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 30 days
Packaging
Please select Package Type and Package Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Work life @25°C
24 hours
Thermal Properties
Glass Transition Temperature (Tg)
46 °C
Thermal Conductivity
4.1 W/m.K
Physical Properties
Thixotropic index
5.8
Viscosity
11,000 mPa.s

Additional Information

Specific Characteristics:

  • High Thermal Conductivity
  • High volume diode (LED) manufacturing
  • Completely supersedes ABP 8037T which has been discontinued
  • Very good on small die
  • Very good on gold (Au) finishing leadframes

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers