LOCTITE ABLESTIK ABP 6392TEA

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE ABLESTIK ABP 6392TEA

Main features

  • High electrical conductivity
  • High thermal conductivity
  • Good adhesion to a variety of substrates

Product Description

LOCTITE ABLESTIK ABP 6392TEA  electrically and thermally conductive, silver filled die attach paste is specially formulated for high reliability packaging applications. ABLESTIK ABP 6392TEA is designed for use on small to large die sizes to balance stress management.

LOCTITE ABLESTIK ABP 6392TEA adhesive is formulated to provide good adhesion on a wide variety of substrates, including Cu, Ag, PP,F and laminate.

 

Cure Schedule

  • 30 minutes ramp to 175°C + 60 minutes @ 175°C, in air or nitrogen
Product Family

ABLESTIK ABP6392TEA

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 23 days
CA Shipping in 2 weeks
EU Shipping in 20 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Work life @25°C
24 hours
Thermal Properties
Glass Transition Temperature (Tg)
56 °C
Thermal Conductivity
9 W/m.K
Electrical Properties
Volume Resistivity
0.00004 Ohms⋅cm
Chemical Properties
Moisture absorption
0.13 %
Physical Properties
Thixotropic index
5
Viscosity
12,500 mPa.s

Additional Information

Recommended Cure Condition

  • 30 minutes ramp to 175°C + 60 minutes @ 175°C, in air or nitrogen.

Thawing

  1. Allow container to reach room temperature before use.
  2. After removing from the freezer, set the syringes to stand vertically while thawing.
  3. Thaw times depend on the syringe size.
  4. Consult handling guide for more information.
  5. DO NOT open the container before contents reach 25°C temperature. Any moisture that collects on the thawed container should be removed prior to opening the container.
  6. DO NOT re-freeze. Once thawed to 25°C, the adhesive should not be re-frozen.

Direction for Use

  1. Thawed material should immediately be placed on dispense equipment for use.
  2. If the adhesive is transferred to a final dispensing reservoir, care must be exercised to avoid entrapment of contaminants and/or air into the adhesive.
  3. Adhesive must be completely used within the product's recommended work life.
  4. Alternate dispense amounts may be used depending on the application requirements.