LOCTITE ABLESTIK ABP 2032S

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Loctite Ablestik ABP 2032S

Main features

  • Low temperature cure
  • Good adhesion
  • Electrically conductive

Product Description

LOCTITE ABLESTIK ABP 2032S electrically conductive epoxy adhesive is designed as a Pb-free alternative to solder. It cures quickly at low temperatures for good stress control in small to medium die applications. It is a tried and proven product for optical sensor ASIC attach and for Lid attach for optical sensors and 3d sensing modules.

LOCTITE ABLESTIK ABP 2032S has good adhesion and good dispensing characteristics, This material can cure in temperatures as low as 80°C and works great on substrates such as Gold, Steel and Silver. 

Cure Schedule

  • 60 minutes @ 80°C
  • 3 minutes @ 150°C or
  • 10 minutes @ 120°C
Product Family

ABLESTIK ABP2032S

1. Select Package Type
2. Select Package Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 30 days
CA Shipping in 12 weeks
EU Shipping in 35 days
Packaging
Please select Package Type and Package Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Work life @25°C
24 hours
Thermal Properties
Thermal Conductivity
1 W/m.K
Physical Properties
Thixotropic index
4.5
Viscosity
11,000 mPa.s