ABLESTIK 970-1N1

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

ABLESTIK 970-1N1

Main features

  • Thixotropic Application Control
  • 20.7 N/mm^2 Aluminum Lap Shear
  • 90-Minute Working Window

Product Description

LOCTITE® ABLESTIK 970-1N1 is a blue, sag-resistant epoxy adhesive for general assembly applications across a wide range of substrates. The material provides a typical mixed viscosity of 60,400 mPa·s, a 90-minute work life at 25°C, and heat-cure options of 2 hours at 70°C or 30 minutes at 100°C. After curing for 2 hours at 70°C, typical aluminum-to-aluminum lap shear strength is 20.7 N/mm². The cured adhesive also has a typical Shore D hardness of 75 and a glass-transition temperature of 83°C.

Key features

  • Sag-resistant consistency: A thixotropic index of 2.0 supports controlled placement before cure.
  • Strong aluminum bonding: Typical aluminum-to-aluminum lap shear strength is 20.7 N/mm² after curing for 2 hours at 70°C.
  • Flexible heat-cure options: Guideline schedules include 2 hours at 70°C or 30 minutes at 100°C.

Applications / Suitable for

  • General assembly bonding
  • Applications requiring sag-resistant adhesive placement
  • Aluminum-to-aluminum bonding under the documented cure condition
Product Family

ABLESTIK 970-1N1

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Blue
Chemistry Type
Epoxy
Specific Gravity
1.06
Work life @25°C
1.5 hours
Thermal Properties
Glass Transition Temperature (Tg)
83 °C
Physical Properties
Thixotropic index
2.0
Viscosity
60400 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties, storage information, and guideline cure schedules for the adhesive before final processing.

Property Value Unit Method / condition
Technology Epoxy — General-purpose adhesive
Appearance Blue liquid — As supplied
Mixed viscosity 60,400 mPa·s (cP) Brookfield CP52, 2.5 rpm
Thixotropic index 2.0 — 1/10 rpm
Specific gravity 1.2 — SDS physical-property value
Work life 90 minutes At 25°C
Cure schedule 2 hours or 30 minutes — 2 hours at 70°C or 30 minutes at 100°C; guideline recommendations
Optimal storage -40 °C Store unopened in a dry location
Technical properties

After-processing / final-state properties

Typical cured-material properties and bonded-joint performance. Values are reference data and are not product specifications.

Property Value Unit Method / condition
Hardness 75 Shore D Cure condition and test method not stated
Specific gravity — cured 1.06 — Test method and cure condition not stated
Glass-transition temperature 83.0 °C TMA, 20°C/minute; cure condition not stated
Coefficient of thermal expansion — Alpha 1 60.0 ppm/°C Temperature range and cure condition not stated
Lap shear strength — aluminum to aluminum 20.7 (3,000) N/mm² (psi) Cured for 2 hours at 70°C; substrate preparation, bondline, and test method not stated