ABLESTIK 967-3

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

ABLESTIK 967-3

Main features

  • 2 x 10^13 ohm-cm Volume Resistivity
  • 6-Hour 65 deg C Cure
  • 1:1 Meter-Mix Processing

Product Description

LOCTITE® ABLESTIK 967-3 is a two-component, electrically insulating epoxy adhesive developed for die-attach applications requiring lower-than-normal cure temperatures. The brownish-gray material mixes at 1:1 by weight and can be applied by automatic dispensing, screen printing, or hand probe. It provides a typical viscosity of 7,000 mPa·s at 25°C and a two-day work life at 25°C. Guideline heat-cure options include 6 hours at 65°C or 30 minutes at 150°C, while typical cured properties include thermal conductivity of 0.7 W/(m·K), volume resistivity of 2 × 1013 ohm-cm, and a glass-transition temperature of 85°C.

Key features

  • Low-temperature die-attach cure: An alternative guideline cure schedule of 6 hours at 65°C supports assemblies requiring reduced cure temperature.
  • Electrically insulating: Typical cured volume resistivity is 2 × 1013 ohm-cm, with a dielectric constant of 4.3 at 1 kHz.
  • Flexible application methods: Suitable for automatic dispensing, screen printing, and hand-probe application.

Applications / Suitable for

  • Die-attach applications
  • Assemblies requiring lower-temperature heat cure
  • Automatic dispensing
  • Screen-printing and hand-probe application
Product Family

ABLESTIK 967-3

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Brownish Grey
Chemistry Type
Epoxy
Mix Ratio
1 : 1
Work life @25°C
48 hours
Thermal Properties
Glass Transition Temperature (Tg)
85 °C
Thermal Conductivity
0.7 W/m.K
Electrical Properties
Volume Resistivity
2×10¹³ Ohms⋅cm
Physical Properties
Viscosity
7000 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties, storage conditions, and guideline cure schedules for the adhesive before final processing.

Property Value Unit Method / condition
Technology Epoxy — Two-component adhesive
Appearance Brownish gray — TDS description
Mix ratio — Part A:Part B 1:1 by weight Equal weights of Parts A and B
Viscosity 7,000 mPa·s (cP) At 25°C; method not stated
Specific gravity 1.7 — SDS physical-property value
Work life 2 days At 25°C
Shelf life — two-component kit 365 days At 5°C, from date of manufacture
Shelf life — two-component kit 183 days At 25°C, from date of manufacture
Shelf life — premixed frozen 365 days At -40°C, from date of manufacture
Cure schedule 30 minutes or 6 hours — 30 minutes at 150°C or 6 hours at 65°C; guideline recommendations
Technical properties

After-processing / final-state properties

Typical cured-material properties and die-attach performance. Values are reference data and are not product specifications.

Property Value Unit Method / condition
Glass-transition temperature 85 °C TMA; cure condition not stated
Thermal conductivity at 121°C 0.7 W/(m·K) Test method, bondline thickness, and orientation not stated
Extractable chloride ≤300 ppm Extractable ionic content; method not stated
Extractable sodium ≤10 ppm Extractable ionic content; method not stated
Extractable potassium ≤30 ppm Extractable ionic content; method not stated
Water-extract conductivity 80 µmhos/cm Test method and extraction conditions not stated
Volume resistivity 2 × 1013 ohm-cm Test method and cure condition not stated
Dielectric constant 4.3 — At 1 kHz
Dissipation factor 0.025 — At 1 kHz
Die shear strength — 2 × 2 mm gold die on gold substrate 11 kg-f Tested at 25°C; cure condition and test method not stated
Lap shear strength — 2 × 2 mm aluminum on aluminum substrate ≥1,700 psi Tested at 25°C; cure condition and test method not stated

Leading Brands Trust in Our Products and Services