LOCTITE ABLESTIK 965-1L

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE ABLESTIK 965-1L

Main features

  • Stress absorbing
  • Low contaminants
  • For large dies

Product Description

LOCTITE ABLESTIK 965-1L is designed for bonding large die integrated circuits with mismatched coefficients of thermal expansion. It is designed for high speed, automated assembly operations.

LOCTITE ABLESTIK 965-1L is a silver filled epoxy that absorbs stress while also claims low levels of contaminants. It offers a void free bond line with minimal bleed.

Cure Schedule

  • 1 hour @ 150°C
Product Family

ABLESTIK 965-1L

1. Select Package Type
2. Select Package Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 25 days
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Package Type and Package Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Work life @25°C
24 hours
Thermal Properties
Glass Transition Temperature (Tg)
72 °C
Thermal Conductivity
3 W/m.K
Electrical Properties
Volume Resistivity
0.0005 Ohms⋅cm
Physical Properties
Thixotropic index
4.5
Viscosity
12,000 mPa.s