LOCTITE ABLESTIK 958-7 | Electrically Conductive Adhesive

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE ABLESTIK 958-7 | Electrically Conductive Adhesive

Main features

  • Electrically conductive
  • Good adhesion to gold
  • Heat cure

Product Description

LOCTITE ABLESTIK 958-7 is a silver-filled, electrically conductive epoxy adhesive engineered for high-reliability hybrid die attach applications. Formulated for advanced electronic assemblies, this adhesive delivers both strong mechanical bonding and consistent electrical performance, even under thermal and environmental stress.

What sets 958-7 apart is its enhanced adhesion to gold surfaces, making it particularly well-suited for sensitive components in hybrid circuits, semiconductors, and high-density electronics. Its proven track record in reliability makes it a go-to solution for manufacturers that demand dependable electrical conductivity along with robust bond strength.

Typical Applications:

  • Hybrid Die Attach
  • High-Reliability Electronics
  • RF and Microwave Components
Product Family

ABLESTIK 958-7

1. Select Package Type
2. Select Package Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 17 days
CA Shipping in 8 weeks
EU Shipping in 35 days
Packaging
Please select Package Type and Package Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Gray
Work life @25°C
168 hours
Electrical Properties
Volume Resistivity
0.0001 Ohms⋅cm
Chemical Properties
Water Extract Conductivity
1.5e-7 Ohm
Physical Properties
Viscosity
90,000 mPa.s
Thermal Properties
Flash Point
93 °C
Glass Transition Temperature (Tg)
67 °C
Thermal Conductivity
2.0 W/m.K
Weight Loss @ 300°C
0.23 %

Additional Information

LOCTITE ABLESTIK 958-7 ADDITIONAL SPECIFICATIONS

Property Value Unit
Lap Shear Strength @25℃ (Al to Al) 14 N/mm2
Bond Strength @25℃ 39 N/mm2
Bond Strength @25℃ (after 1,000 hours @150℃) 37 N/mm2

Recommended Cure Schedule

  • 1 hour @150°C

Thawing

  1. Allow container to reach room temperature before use.
  2. After removing from the freezer, set the syringes to stand vertically while thawing.
  3. DO NOT open the container before contents reach 25°C temperature. Any moisture that collects on the thawed container should be removed prior to opening the container.
  4. DO NOT re-freeze. Once thawed to 25°C, the adhesive should not be re-frozen.

Loctite ablestik 958-7 Thawing Curve

Directions for Use

  1. Thawed adhesive should immediately be placed on dispense equipment for use.
  2. If the adhesive is transferred to a final dispensing reservoir, care must be exercised to avoid entrapment of contaminants and/or air into the adhesive.
  3. Adhesive must be completely used within the product's recommended work life.
  4. Apply enough adhesive to achieve a 25 to 50 µmwet bondline thickness, dispensed with approximately 25 to 50 % filleting on all sides of the die.
  5. Alternate dispense amounts may be used depending onthe application requirements.
  6. Star or crossed shaped dispense patterns will yield fewerbondline voids than the matrix style of dispense pattern.