LOCTITE ABLESTIK 84-3

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

Loctite Ablestik 84-3

Main features

  • Solvent-free
  • Aerospace applications
  • Bonds to multiple substrates

Product Description

LOCTITE ABLESTIK 84-3 non conductive adhesive is designed for medium size die attach and assembly applications. This adhesive is ideal for application by automatic dispensing, screen printing or hand. It has fairly high viscosity and can be applied by dispense or print while also resisting air expansion. Additionally, it is epoxy-based, so should bond well to almost any surface. It's poison ration is estimated at ±0.3 which is typical for epoxy adhesives.

LOCTITE ABLESTIK 84-3 is based on the tried and true 84-1LMI chemistry, has a well defined operating temperature range and is well accepted in military/defense applications for several years. It meets the requirements of MIL-STD-883, Method 5011 and passes NASA outgassing standards if cured properly but is epoxy based and is unlikely to survive the AuSn reflow process.
The weight loss of 84-3 at 300 °C is only 0.17%, but the properties, performance, and reliability after the AuSn reflow profile would have to be tested. 

 

Cure Schedule

  • 1 hour @ 150°C
  • 2 hours @ 125°C
Product Family

ABLESTIK 84-3

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 28 days
CA Shipping in 12 weeks
EU Shipping in 50 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Density (g)
1.7 g/cm3
Work life @25°C
336 hours
Thermal Properties
Glass Transition Temperature (Tg)
85 °C
Thermal Conductivity
0.8 W/m.K
Weight Loss @ 300°C
0.17 %
Physical Properties
Thixotropic index
14
Viscosity
50,000 mPa.s