LOCTITE ABLESTIK 8387BS
Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg
Main features
- Non conductive
- Contains spacers
- Black pigmentation
Product Description
LOCTITE 8387BS single component adhesive is designed for high throughput bonding applications. It contains spacers for improved bondline control.
LOCTITE 8387BS is a non conductive, black epoxy that blocks the stray light and has 30um polymer spacers to control the bondline thickness.
Cure Schedule
- 1 hour @ 100°C
- 90 minutes @ 90°C
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Work life @25°C
48 hours
Thermal Properties
Glass Transition Temperature (Tg)
122 °C
Physical Properties
Thixotropic index
4.5
Viscosity
14,250 mPa.s