LOCTITE ABLESTIK 8290

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Loctite Ablestik 8290

Main features

  • Low bleed
  • Low stress
  • Improved JEDEC performance

Product Description

LOCTITE® ABLESTIK 8290 electrically conductive die attach adhesive is designed for high reliability leadframe packaging applications. It is recommended for die sizes smaller than 5mm for the best MRT performance.

LOCTITE® ABLESTIK 8290 is an epoxy based, silver filled, heat curable adhesive with low bleed and low stress that also achieves improved JEDEC performance.

 

Cure Schedule

  • 30 minute ramp to 175°C + 15 minutes @ 175°C
Product Family

ABLESTIK 8290

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 30 days
CA Shipping in 12 weeks
EU Shipping in 55 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Work life @25°C
24 hours
Thermal Properties
Thermal Conductivity
8 W/m.K
Physical Properties
Thixotropic index
4.0
Viscosity
16,000 mPa.s