LOCTITE ABLESTIK 8008

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Loctite Ablestik 8008HT

Main features

  • Snap curable after B stage
  • Low modulus
  • Void free bondline without bleed

Product Description

LOCTITE® ABLESTIK 8008 snap curable adhesive is designed for small die sizes (an be applied to a wafer backside by stencil printing and then B-staged in an oven. The adhesive can then be cured after die attach in an in-line process exhibiting a consistent, void-free bondline without bleed.

LOCTITE ABLESTIK 8008 should be used with a pressure sensitive dicing tape and is not compatible with UV dicing tapes.

Product Family

ABLESTIK 8008

No longer available

This product is no longer available from Krayden. Please contact us so we can recommend an alternative product.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Work life @25°C
24 hours
Thermal Properties
Glass Transition Temperature (Tg)
270 °C
Thermal Conductivity
2.2 W/m.K
Physical Properties
Thixotropic index
2.6
Viscosity
48,000 mPa.s