LOCTITE ABLESTIK 789-3

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE ABLESTIK 789-3

Main features

  • Non conductive
  • Good moisture resistance
  • Substrate attach

Product Description

LOCTITE ABLESTIK 789-3 die attach adhesive is designed for microelectronic applications. This adhesive exhibits strong adhesion to difficult-to-bond metals and retains its bond strength after exposure to moisture.

LOCTITE ABLESTIK 789-3 is a non conductive epoxy adhesive with good moisture resistance and high bond strength. It is typically used for substrate attach and package sealing on gold, silver and copper substrates.

Cure Schedule

  • 30 minutes @ 150°C 
  • 4 hours @ 93°C
Product Family

ABLESTIK 789-3

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 20 days
CA Shipping in 12 weeks
EU Shipping in 40 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Work life @25°C
2184 hours
Thermal Properties
Glass Transition Temperature (Tg)
126 °C
Thermal Conductivity
0.3 W/m.K
Weight Loss @ 300°C
0.28 %
Electrical Properties
Volume Resistivity
2000000000000000 Ohms⋅cm
Physical Properties
Viscosity
36,500 mPa.s