ABLESTIK 642-1

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

ABLESTIK 642-1

Main features

  • Extended 8-Hour Assembly Window
  • Multiple Heat-Cure Schedules
  • Low-Outgassing Assembly Bonding

Product Description

LOCTITE ABLESTIK 642-1 is a one-part, transparent, unfilled epoxy adhesive for general assembly bonding. It combines an 8-hour work life at 25 deg C with elevated-temperature cure options of 2 hours at 75 deg C, 1 hour at 95 deg C, or 30 minutes at 120 deg C. The cured adhesive has a typical Shore D hardness of 87 and aluminum-to-aluminum lap shear strength of 19.3 N/mm^2 at 25 deg C. The formulation passes NASA outgassing standards, making it relevant to assemblies that require controlled outgassing alongside heat-cure processing.

Key features

  • Extended assembly window: An 8-hour work life at 25 deg C provides time for adhesive application and part positioning.
  • Multiple elevated-temperature cures: Three cure schedules allow selection between lower-temperature processing and a faster 30-minute cycle.
  • Low-outgassing performance: The formulation passes NASA outgassing standards for assemblies that require controlled outgassing.

Applications

Applications include general assembly bonding and heat-cured assemblies that require low-outgassing performance.

Product Family

ABLESTIK 642-1

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Transparent liquid
Component System
One-component
Work life @25°C
8 hours
Physical Properties
Thixotropic index
1.0
Viscosity
5,500 mPa.s
Thermal Properties
Glass Transition Temperature (Tg)
137.0 °C
Electrical Properties
Volume Resistivity
6.50×10¹⁴ Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Technical values are typical; the listed cure schedules are guideline recommendations.

PropertyValueUnitMethod / condition
AppearanceTransparent liquidAs supplied
Viscosity5,500mPa s25 deg C
Thixotropic index1.0Typical
Work life8hours25 deg C
Shelf life, pre-mixed frozen365days-40 deg C
Shelf life, kits365days25 deg C
Cure schedule2 at 75; 1 at 95; 0.5 at 120hours at deg CGuideline heat-cure options
Technical properties

After-processing / final-state properties

Values are typical for cured LOCTITE ABLESTIK 642-1 under the stated conditions.

PropertyValueUnitMethod / condition
Shore D hardness87Typical cured material
Glass transition temperature137.0deg CTypical cured material
Coefficient of thermal expansion84ppm/deg CTypical cured material
Volume resistivity6.50 x 10^14ohm cm100 deg C
Dielectric constant3.361 kHz
Dissipation factor0.0071 kHz
Lap shear strength19.3N/mm^2Aluminum-to-aluminum; 25 deg C