LOCTITE ABLESTIK 550K
Harmonization Code : 3920.99.28.90 | Other plates, sheets, film, foil and strip, of plastics, non-cellular and not reinforced, laminated, supported or similarly combined with other materials ; Of other plastics ; Other; Other
Main features
- Low cure temperature
- Hard to bond metals
- Thermally conductive
Product Description
LOCTITE ABLESTIK 550K is a white epoxy film designed for substrate attach and heat sink bonding. It offers high thermal conductivity and low cure temperature and comes on a glass fabric carrier.
LOCTITE ABLESTIK 550K is a non-electrically conductive, epoxy assembly film commonly used on Gold and gold plated surfaces and is suitable for an array of difficult-to-bond metals.
Cure Schedule
- 30min @150°C
- 2 hours @ 125°C
Packaging
Please select Package Type and Thickness.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Work life @25°C
4392 hours
Thermal Properties
Glass Transition Temperature (Tg)
102 °C
Thermal Conductivity
0.8 W/m.K
Weight Loss @ 300°C
0.37 %
Electrical Properties
Volume Resistivity
7200000000000 Ohms⋅cm