ABLESTIK 5074

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

ABLESTIK 5074

Main features

  • Flexible Dissimilar-Material Bonding
  • Multiple Heat-Cure Options
  • Reworkable Non-Conductive Film

Product Description

LOCTITE ABLESTIK 5074 is a configurable, non-conductive epoxy adhesive film reinforced with glass fabric for electronics assembly. The flexible, reworkable film is used across mixed-material interfaces, with thickness and dimensions selected for the supplied configuration. It has a 24-hour work life at 25 deg C and can be heat cured for 180 minutes at 100 deg C, 90 minutes at 125 deg C, or 60 minutes at 150 deg C. The cured material has a typical thermal conductivity of 0.9 W/(m K). It is supplied as sheet stock or die-cut preforms.

Key features

  • Flexible mixed-material film: Bonds dissimilar materials with differing coefficients of thermal expansion in electronics assemblies.
  • Multiple heat-cure options: Three supported time-and-temperature schedules provide practical cure flexibility for the assembly process.
  • Reworkable non-conductive construction: Provides a non-conductive film bond in a format intended for assemblies that may require rework.

Applications

Applications include electronics assembly bonding of dissimilar materials with differing coefficients of thermal expansion.

Product Family

ABLESTIK 5074

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
White
Work life @25°C
24 hours
Thermal Properties
Glass Transition Temperature (Tg)
3 °C
Thermal Conductivity
0.9 W/m.K

Additional Information

Technical properties

As-supplied / before-processing properties

Supplied thickness and dimensions depend on the selected sheet or die-cut configuration.

PropertyValueUnitMethod / condition
AppearanceWhiteAs supplied
Film constructionEpoxy-coated glass fabricConfigurable 5074 family
Work life24hours25 deg C
Shelf life183days-40 deg C; from date of manufacture
Available formsSheet stock or die-cut preformsThickness and dimensions are configuration-specific
Cure schedule180 at 100; 90 at 125; 60 at 150minutes at deg CGuideline heat-cure options
Technical properties

After-processing / final-state properties

Final-state values are typical for the cured 5074 family material and the stated test configurations.

PropertyValueUnitMethod / condition
Coefficient of thermal expansion, below Tg45ppm/deg CTypical
Coefficient of thermal expansion, above Tg350ppm/deg CTypical
Glass transition temperature3deg CTypical
Thermal conductivity0.9W/(m K)Laser flash
Lap shear strength8N/mm^2Aluminum-to-aluminum; 25 deg C
Lap shear strength5N/mm^2Gold-to-gold; 25 deg C