LOCTITE ABLESTIK 3888

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE ABLESTIK 3888 LOCTITE ABLESTIK 3888

Main features

  • Repair kit
  • Two component silver epoxy
  • Repair/Rework interconnections

Product Description

LOCTITE ABLESTIK 3888 is a two part epoxy paste, designed for bonding of metals, ceramics, rubbers and plastics as used in electronic parts, where good adhesion combined with electrical and thermal conductivity is required. It contains a resin and a hardener and can cure either in room temperature or with heat.

LOCTITE ABLESTIK 3888 has many practical applications which include and are not limited to solder replacement, repair/rework of interconnections, and bonding of heat sensitive components where solder temperatures are impractical. It can withstand operating temperatures up to 80°C.

Cure Schedule:

  • 24 hours @ 23 °C
  • 2 hours @ 65 °C
  • 1 hour @ 125 °C
  • 30 minutes @ 150 °C
Product Family

ABLESTIK 3888

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 15 days
CA Shipping in 12 weeks
EU Shipping in 40 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Pot Life
1.5 hours
Specific Gravity
2.5
Thermal Properties
Glass Transition Temperature (Tg)
50 °C
Thermal Conductivity
1.5 W/m.K
Electrical Properties
Volume Resistivity
0.0001 Ohms⋅cm

Additional Information

What is a Twinpak?


TwinPaks are part A and B in the same package, separated by a plastic bar. (think of it like what you do to seal half-eaten bags of potato chips). The bar (once removed) is then used to mix A and B together. Once they are mixed, the corner of the pack is cut and the "b-stage epoxy" is applied to the part.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers