ABLESTIK 281

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

ABLESTIK 281

Main features

  • Non-Sag Placement Control
  • 1 x 10^15 ohm-cm Volume Resistivity
  • 55 to 180 deg C Service Range

Product Description

LOCTITE® ABLESTIK 281 BK is a one-component, heat-cured epoxy adhesive formulated for assembly applications requiring thermal conductivity and electrical insulation. The black, thixotropic, non-sag paste is documented for bonding metals, glass, and plastics and provides controlled placement with minimal flow. Guideline cure schedules range from 4 hours at 80°C to 15 minutes at 180°C. Typical cured properties include thermal conductivity of 1.4 W/(m·K), volume resistivity above 1 × 1015 ohm-cm at 25°C, and an operating-temperature range of -55 to 180°C.

Key features

  • Thermally conductive and electrically insulating: Typical cured thermal conductivity is 1.4 W/(m·K), with volume resistivity above 1 × 1015 ohm-cm at 25°C.
  • Thixotropic, non-sag paste: Supports controlled adhesive placement with reduced flow during assembly.
  • Wide heat-cure window: Guideline schedules include 4 hours at 80°C, 1 hour at 120°C, 30 minutes at 150°C, or 15 minutes at 180°C.

Applications / Suitable for

  • Assembly bonding
  • Applications requiring thermal conductivity and electrical insulation
  • Bonding metals, glass, and plastics
Product Family

ABLESTIK 281

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Black thixotropic paste
Chemistry Type
Epoxy
Density (g)
2.3 g/cm3
Thermal Properties
Operating Temperature
-55 to +180 °C
Thermal Conductivity
1.4 W/m.K
Chemical Properties
Water Absorption
0.06 %
Electrical Properties
Volume Resistivity
>1×10¹⁵ Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical physical, storage, and guideline cure information for the adhesive before final processing.

Property Value Unit Method / condition
Technology Epoxy — One-component, heat-cured adhesive
Appearance Black thixotropic paste — As supplied
Density 2.3 g/cm³ TDS typical value; SDS reports specific gravity of 2.35
Shelf life 3 months At 25°C, from date of manufacture
Recommended cure schedule 4 hours At 80°C; guideline recommendation
Alternative cure schedules 1 hour, 30 minutes, or 15 minutes — 1 hour at 120°C, 30 minutes at 150°C, or 15 minutes at 180°C; guideline recommendations
Optimal storage 25 °C Store unopened in a dry location; SDS states storage at or below 25°C
Technical properties

After-processing / final-state properties

Typical cured thermal, electrical, mechanical, moisture-exposure, and outgassing properties. Values are reference data and are not product specifications.

Property Value Unit Method / condition
Operating-temperature range -55 to 180 °C Documented product range
Hardness 88 Shore D Cure condition and test method not stated
Coefficient of thermal expansion 32.4 ppm/°C TMA
Thermal conductivity 1.4 W/(m·K) ASTM D2214
Water absorption 0.06 % After 24-hour boil
Volume resistivity >1 × 1015 ohm-cm At 25°C; test method not stated
Total mass loss 0.35 % TML per NASA Reference Publication 1124; sample cured 5 hours at 80°C
Collected volatile condensable material 0.06 % CVCM per NASA Reference Publication 1124; sample cured 5 hours at 80°C
Flexural strength 62 (9,000) N/mm² (psi) ASTM D790
Compressive strength 83 (12,000) N/mm² (psi) Test method not stated
Tensile lap shear strength — aluminum to aluminum at 25°C 13.8 (2,000) N/mm² (psi) Surface preparation, bondline, cure condition, and test method not stated
Tensile lap shear strength — aluminum to aluminum at 120°C 9 (1,300) N/mm² (psi) Surface preparation, bondline, cure condition, and test method not stated