ABLESTIK 24

Harmonization Code : 5906100000 | Adhesive tape of a width not exceeding 20cm

ABLESTIK 24

Main features

  • Water-Clear Thin-Bondline Adhesive
  • 30-Minute Pot Life
  • Flexible Cured Adhesive

Product Description

LOCTITE® ABLESTIK 24 is a water-clear, two-part epoxy adhesive for non-electrically conductive assembly bonding. It is recommended for joining transparent materials such as glass and for applications where a thin bond line is desired. The mixed adhesive has a viscosity of 800 mPa·s at 25 °C and a 30-minute pot life in 50 g quantities. It cures at room temperature, with full properties developed in 16 to 24 hours, and forms flexible, resilient bonds between materials with mismatched coefficients of thermal expansion.

Key features

  • Water-clear epoxy system: Supports transparent-material bonding where adhesive appearance and thin bond lines are important.
  • Room-temperature cure: Two-part system cures at 25 °C, with full properties developed in 16 to 24 hours.
  • Flexible cured adhesive: Forms resilient bonds between materials with mismatched coefficients of thermal expansion.

Applications / Suitable for

  • Joining transparent materials such as glass
  • Thin bond-line adhesive assembly
  • Non-electrically conductive bonding of metals, ceramics, polycarbonate, polystyrene, polysulfone, and rigid plastics
Product Family

ABLESTIK 24

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Mix Ratio
100:28
Pot Life
30 minutes
Thermal Properties
Thermal Conductivity
0.2 W/m.K
Electrical Properties
Dielectric Strength
16.5 kV/mm
Volume Resistivity
1E14 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the mixed two-part adhesive before final cure.

Property Value Unit Method / condition
Technology Epoxy — Two-component adhesive system
Appearance Water clear — As supplied / mixed adhesive appearance
Mix ratio 100:28 — Part A:Part B by weight
Mixed viscosity 800 mPa·s Mixed material at 25°C
Pot life 30 minutes At 25°C, 50 g quantities
Cure schedule 1 to 3 hours At 25°C; full properties develop in 16 to 24 hours
Optimal storage 18 to 25 °C Store in original, tightly covered containers in clean, dry areas
Technical properties

After-processing / final-state properties

Typical values for the cured adhesive after room-temperature cure.

Property Value Unit Method / condition
Tensile lap shear strength 12 N/mm² Typical performance of cured material
Thermal conductivity 0.2 W/(m·K) Typical cured-material physical property
Coefficient of linear thermal expansion 60 ppm/°C Typical cured-material physical property
Volume resistivity 1 × 10¹⁴ ohm-cm At 25°C
Dielectric strength 16.5 kV/mm ASTM D149
Operating temperature 90 continuous; 120 intermittent °C Cured adhesive service exposure