ABLESTIK 2248

Harmonization Code : 5906100000 | Adhesive tape of a width not exceeding 20cm

ABLESTIK 2248

Main features

  • Thixotropic Application Control
  • 14.8 kV/mm Dielectric Strength
  • 1-Hour Working Window

Product Description

LOCTITE® ABLESTIK 2248 BIPAX is a two-component, heat-cured epoxy staking compound supplied in a mixing-dispenser package. The tan, thixotropic system mixes at 100:19.4 resin-to-hardener by weight and is documented for bonding metals, glass, ceramics, and plastics. It combines toughness, impact resistance, thermal-shock resistance, and low permeability to gases and vapors with a two-hour pot life and a guideline cure schedule of 1 hour at 100°C. Typical cured properties include an operating-temperature range of -60 to 190°C, Shore D hardness of 87, tensile strength of 72.4 N/mm², and volume resistivity of 2.50 × 1015 ohm-cm at 25°C.

Key features

  • Tough, thermally durable system: Documented for good toughness, impact resistance, thermal-shock resistance, and service from -60 to 190°C.
  • Controlled thixotropic handling: Typical mixed viscosity is 10,000 mPa·s at 25°C with a two-hour pot life.
  • Electrical insulation: Typical cured volume resistivity is 2.50 × 1015 ohm-cm at 25°C, with dielectric strength of 14.8 kV/mm.

Applications / Suitable for

  • Staking applications
  • Bonding metals, glass, ceramics, and plastics
  • Assemblies exposed to thermal shock or elevated service temperatures
  • Applications requiring low permeability to gases and vapors
Product Family

ABLESTIK 2248

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Tan
Chemistry Type
Epoxy
Mix Ratio
100 : 19.4
Pot Life
2 hours
Specific Gravity
1.2
Thermal Properties
Glass Transition Temperature (Tg)
109.0 °C
Operating Temperature
-60 to 190 °C
Mechanical Properties
Elongation
2 %
Chemical Properties
Water Absorption
0.001 %
Electrical Properties
Dielectric Strength
14.8 kV/mm
Volume Resistivity
2.50×10¹⁵ Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical mixed, handling, storage, and guideline cure information before final processing.

Property Value Unit Method / condition
Technology Epoxy — Two-component heat-cured staking compound
Appearance — mixed Tan — Uniformly mixed BIPAX system
Appearance — resin Light yellow liquid — LOCTITE ABLESTIK 2248-R SDS
Appearance — hardener Amber to brown liquid — LOCTITE ABLESTIK 2248-H SDS
Mix ratio — resin:hardener 100:19.4 by weight Documented BIPAX mix ratio
Mixed viscosity 10,000 mPa·s (cP) Brookfield LV, spindle 4, 12 rpm at 25°C
Specific gravity — mixed 1.2 — Typical mixed value
Specific gravity — resin 1.3 — LOCTITE ABLESTIK 2248-R SDS
Specific gravity — hardener 1.0 — LOCTITE ABLESTIK 2248-H SDS
Pot life 2 hours Temperature and test mass not stated
Guideline cure schedule 1 hour At 100°C
Application-dependent post-cure 2 hours At 125°C when anticipated application temperatures exceed 125°C
Optimal storage ≤27 °C TDS storage value; component SDSs specify storage at or below 25°C
Technical properties

After-processing / final-state properties

Typical cured physical, thermal, electrical, outgassing, and bonded-joint properties. Values are reference data and are not product specifications.

Property Value Unit Method / condition
Operating-temperature range -60 to 190 °C Documented product range
Hardness 87 Shore D Cure condition and test method not stated
Glass-transition temperature 109 °C Method and cure condition not stated
Coefficient of expansion 50 ppm/°C Temperature range, method, and cure condition not stated
Heat-distortion temperature 148 °C Method and cure condition not stated
Water absorption 0.001 % After 24-hour immersion
Izod impact strength 0.52 ft-lb/in of notch Test method and cure condition not stated
Elongation 2 % Test method and cure condition not stated
Dielectric strength 14.8 kV/mm Test method, specimen thickness, and cure condition not stated
Dielectric constant 4.35 — At 1 kHz and 25°C
Dissipation factor 0.02 — At 1 kHz and 25°C
Volume resistivity 2.50 × 1015 ohm-cm At 25°C
Outgassing Passes — ASTM E595-90
Lap shear strength — aluminum to aluminum 17.9 (2,600) N/mm² (psi) Surface preparation, bondline, cure condition, test method, and test temperature not stated
Tensile strength 72.4 (10,500) N/mm² (psi) Test method and cure condition not stated