ABLESTIK 2143D

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

ABLESTIK 2143D

Main features

  • Medium-Viscosity Application Control
  • 1 x 10^14 ohm-cm Volume Resistivity
  • Room-Temperature Adhesive Cure

Product Description

LOCTITE® ABLESTIK 2143D is a two-component, medium-viscosity epoxy adhesive for industrial bonding and sealing applications requiring toughness, impact resistance, and electrical insulation. The amber system mixes at a 100:100 resin-to-hardener ratio by weight and bonds most metals, rigid plastics, ceramics, glass, leather, rubber, wood, and concrete. The mixed adhesive has a typical viscosity of 38,000 mPa·s at 25°C and can cure for 24 to 72 hours at 25°C or 4 hours at 65°C. Typical cured properties include a -60 to 100°C operating-temperature range, volume resistivity of 1 × 1014 ohm-cm at 25°C, and aluminum lap shear strength of 15 N/mm².

Key features

  • Tough, impact-resistant bonding: The cured epoxy has a typical Izod impact strength of 1.14 ft-lb/in of notch and is documented for thermal-shock resistance.
  • Electrical insulation: Typical cured volume resistivity is 1 × 1014 ohm-cm at 25°C, with dielectric strength of 460 V/mil.
  • Room-temperature or heat cure: Guideline cure schedules include 24 to 72 hours at 25°C or 4 hours at 65°C.

Applications / Suitable for

  • Industrial bonding and sealing
  • Bonding most metals, rigid plastics, ceramics, and glass
  • Bonding leather, rubber, wood, and concrete
  • Assemblies requiring toughness, impact resistance, or low-temperature performance
Product Family

ABLESTIK 2143D

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Epoxy
Color
Amber
Mix Ratio
100 : 100
Specific Gravity
1.12
Thermal Properties
Glass Transition Temperature (Tg)
65 °C
Operating Temperature
-60 to 100 °C
Physical Properties
Thixotropic index
1.0
Chemical Properties
Water Absorption
0.004 %
Electrical Properties
Volume Resistivity
1×10¹⁴ Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical component, mixed, working-time, storage, and guideline cure information before final processing.

Property Value Unit Method / condition
Technology Epoxy — Two-component adhesive system
Appearance — mixed Amber — Uniformly mixed adhesive
Appearance — resin Light yellow liquid — LOCTITE ABLESTIK 2143D-R
Appearance — hardener Amber liquid — LOCTITE ABLESTIK 2143D-H
Mix ratio — resin:hardener 100:100 by weight Documented system mix ratio
Mixed viscosity 38,000 mPa·s (cP) At 25°C; test method not stated
Thixotropic index 1.0 — As mixed; method not stated
Specific gravity — mixed 1.12 — Typical mixed value
Density / relative density — resin 1.17 — LOCTITE ABLESTIK 2143D-R SDS
Density / relative density — hardener 0.97 — LOCTITE ABLESTIK 2143D-H SDS
Pot life 1 hour 25 g mass; temperature not stated
Pot life 30 minutes 100 g mass; temperature not stated
Work life 1.5 hours 25 g mass; temperature and endpoint not stated
Work life 30 minutes 100 g mass; temperature and endpoint not stated
Recommended cure schedule 24–72 hours At 25°C; guideline recommendation
Alternative cure schedule 4 hours At 65°C; guideline recommendation
Storage ≤27 °C Dry storage in original, sealed, unopened containers; unless otherwise specified on packaging
Technical properties

After-processing / final-state properties

Typical physical, electrical, environmental-exposure, and bonded-joint properties of the cured adhesive. Values are reference data and are not product specifications.

Property Value Unit Method / condition
Operating-temperature range -60 to 100 °C Documented product range
Hardness 77 Shore D Test method and cure condition not stated
Glass-transition temperature 65 °C Ultimate Tg; test method and cure condition not stated
Coefficient of expansion 6.4 × 10-5 cm/cm/°C Temperature range, test method, and cure condition not stated
Reactive solids content 100 % Typical cured-material value
Water absorption 0.004 % After 24 hours; exposure conditions and test method not stated
Izod impact strength 1.14 ft-lb/in of notch Test method and cure condition not stated
Volume resistivity 1 × 1014 ohm-cm At 25°C; test method and cure condition not stated
Dielectric strength 460 V/mil Test method, specimen thickness, conditioning, and cure condition not stated
Dielectric constant 3.35 — At 1 kHz and 25°C
Dissipation factor 0.01 — At 1 kHz and 25°C
Lap shear strength — aluminum to aluminum 15 (2,200) N/mm² (psi) After curing for 1 hour at 65°C; test temperature, surface preparation, bondline, and test method not stated

Leading Brands Trust in Our Products and Services