ABLESTIK 2135D

Harmonization Code : 5906100000 | Adhesive tape of a width not exceeding 20cm

ABLESTIK 2135D

Main features

  • Tough, Durable Epoxy for Bonding, Laminating, Sealing
  • 1,200 mPa s Mixed Viscosity
  • 2.7 x 10^13 ohm-cm Volume Resistivity

Product Description

LOCTITE® ABLESTIK 2135D BIPAX is a two-component, medium-viscosity epoxy adhesive for bonding, laminating, sealing, and structural repair. The light-amber system mixes at 100:60 resin-to-hardener by weight and is documented for bonding metals, ceramics, wood, concrete, phenolics, polyester, epoxy, many urethanes, and other plastics. It provides good wetting, high impact strength, and strong mechanical, shock, and environmental resistance after cure. The mixed adhesive has a typical viscosity of 1,200 mPa·s at 25°C, a 60-minute pot life, and can cure for 24 hours at 25°C or 4 hours at 65°C.

Key features

  • Tough, impact-resistant bonding: Designed to provide high impact strength with mechanical and shock resistance after full cure.
  • Low mixed viscosity and good wetting: Typical mixed viscosity is 1,200 mPa·s at 25°C for application across a broad range of substrates.
  • Room-temperature or heat cure: Guideline schedules include 24 hours at 25°C or 4 hours at 65°C.

Applications / Suitable for

  • Bonding and laminating
  • Sealing and structural repair
  • Bonding metals, ceramics, wood, and concrete
  • Bonding phenolics, polyester, epoxy, many urethanes, and other plastics
Product Family

ABLESTIK 2135D

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Epoxy
Color
Light amber
Mix Ratio
100 : 60
Pot Life
60 minutes
Specific Gravity
1.11
Thermal Properties
Glass Transition Temperature (Tg)
54 °C
Operating Temperature
-60 to 100 °C
Electrical Properties
Volume Resistivity
2.7×10¹³ Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical component, mixed, storage, and guideline cure information before final processing.

Property Value Unit Method / condition
Technology Epoxy — Two-component adhesive system
Appearance — mixed Light amber — Uniformly mixed BIPAX system
Appearance — resin Yellow liquid — LOCTITE ABLESTIK 2135D-R SDS
Appearance — hardener Tan liquid — LOCTITE ABLESTIK 2135D-H SDS
Mix ratio — resin:hardener 100:60 by weight Documented BIPAX mix ratio
Mixed viscosity 1,200 mPa·s (cP) At 25°C; test method not stated
Specific gravity — mixed 1.11 — Typical TDS value
Specific gravity — resin 1.13 — LOCTITE ABLESTIK 2135D-R SDS
Specific gravity — hardener 0.95 — LOCTITE ABLESTIK 2135D-H SDS
Pot life 60 minutes Temperature, test mass, and endpoint not stated
Recommended cure schedule 24 hours At 25°C; guideline recommendation
Alternative cure schedule 4 hours At 65°C; guideline recommendation
Storage ≤27 °C Dry storage in original, sealed, unopened containers unless otherwise specified on packaging
Technical properties

After-processing / final-state properties

Typical physical, electrical, and bonded-joint properties of the cured adhesive. Values are reference data and are not product specifications.

Property Value Unit Method / condition
Operating-temperature range -60 to 100 °C Documented product range
Hardness 70 Shore D Test method and cure condition not stated
Glass-transition temperature 54 °C Ultimate Tg; test method and cure condition not stated
Coefficient of expansion 5.5 × 10-5 cm/cm/°C Temperature range, method, and cure condition not stated
Reactive solids content 100 % Typical TDS value
Volume resistivity 2.7 × 1013 ohm-cm At 25°C; test method and cure condition not stated
Dielectric strength 435 V/mil Test method, specimen thickness, conditioning, and cure condition not stated
Dielectric constant 3.68 — At 1 kHz and 25°C
Dissipation factor 0.02 — At 1 kHz and 25°C
Lap shear strength — aluminum to aluminum 1.61 (234) N/mm² (psi) After curing for 24 hours at 25°C; test temperature, surface preparation, bondline, and method not stated
Lap shear strength — aluminum to aluminum 20 (2,888) N/mm² (psi) After curing for 4 hours at 65°C; test temperature, surface preparation, bondline, and method not stated

Leading Brands Trust in Our Products and Services