LOCTITE ABLESTIK 2114

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE ABLESTIK 2114

Main features

  • Optically Clear Bonding
  • 50 N/mm^2 Cured Tensile Strength
  • Broad Metal/Glass/Ceramic/Plastic Compatibility

Product Description

LOCTITE ABLESTIK 2114 BIPAX is a two-component, transparent, non-conductive epoxy adhesive supplied in a BIPAX mixing-dispenser package for easy mixing. Formulated for optical clarity and low viscosity, it is recommended for industrial adhesive and laminating applications. This solvent-based system cures at room temperature over 24 hours or with an accelerated schedule, and supports continuous service from -60°C to 110°C. It bonds metals, glass, glass fabrics, ceramics, and plastics, offering strong tensile strength, good electrical insulation, and environmental and chemical resistance in its cured state.

Key features

  • Transparent with optical clarity: Low viscosity and refractive index of 1.57 for optically clear bonding applications.
  • High tensile strength: 50 N/mm² (7,200 psi) tensile strength in the cured state.
  • Electrically insulating: Dielectric strength of 410 volts/mil supports non-conductive assembly needs.

Applications / Suitable for: Industrial adhesive and laminating applications across metals, glass, glass fabrics, ceramics, and plastics.

Product Family

ABLESTIK 2114

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Transparent
Refractive index
1.57
Specific Gravity
1.17
Physical Properties
Viscosity
640 mPa.s
Thermal Properties
Glass Transition Temperature (Tg)
77 °C
Operating Temperature
-60 to 110 °C
Electrical Properties
Volume Resistivity
3.5000000000 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of the uncured, mixed material prior to cure.

Property Value Unit Method / condition
Viscosity, mixed 640 mPa·s (cP) @ 25°C, mixed
Specific gravity, mixed 1.17 — Mixed material
Pot life 60 minutes Mixed material
Technical properties

After-processing / final-state properties

Typical properties of the fully cured material after the recommended cure schedule.

Property Value Unit Method / condition
Hardness 78 Shore D Cured material
Glass transition temperature (Tg) 77.0 °C Cured material
Dielectric strength 410 volts/mil Cured material
Tensile strength 50 (7,200) N/mm² (psi) Cured material
Lap shear strength, Al to Al 16.2 (2,350) N/mm² (psi) Sample cured 1 hr @ 100°C