LOCTITE ABLESTIK 2113

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

LOCTITE ABLESTIK 2113

Main features

  • Low-Viscosity Optical Bonding
  • Fine-Detail Flow and Wetting
  • Electrically Insulating Cured Adhesive

Product Description

LOCTITE ABLESTIK 2113 BIPAX is a two-component, transparent, non-conductive epoxy adhesive supplied at a 100:11 resin-to-hardener mix ratio in a BIPAX mixing-dispenser package. Formulated for applications requiring low initial viscosity and near-transparent color, it offers excellent flow and wetting properties for fine detail work and difficult-to-reach bond lines. This solvent-free system cures at room temperature over 24 hours or faster at 65°C, and supports continuous service from -60°C to 130°C. It is recommended for fiber optic assembly, structural laminating, and high-performance aerospace and electronic applications, bonding glass, ceramics, metals, and plastics with good chemical resistance and electrical insulation.

Key features

  • Low viscosity, transparent: 300 mPa·s mixed viscosity with near-transparent cured appearance for optical clarity needs.
  • Excellent flow and wetting: Supports fine detail bonding and fiber optic assembly applications.
  • Electrically insulating: Dielectric strength of 410 volts/mil for demanding electronic applications.

Applications / Suitable for: Fiber optic assembly, structural laminating, and high-performance aerospace and electronic applications.

Product Family

ABLESTIK 2113

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Transparent
Specific Gravity
1.16
Physical Properties
Thixotropic index
1
Viscosity
300 mPa.s
Thermal Properties
Glass Transition Temperature (Tg)
77 °C
Operating Temperature
-60 to 130 °C
Electrical Properties
Volume Resistivity
60000000000000 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of the uncured, mixed material prior to cure.

Property Value Unit Method / condition
Mix ratio (Resin : Hardener) 100 : 11 by weight —
Viscosity, mixed 300 mPa·s (cP) @ 25°C, mixed
Specific gravity, mixed 1.16 — Mixed material
Pot life 30 minutes Mixed material
Technical properties

After-processing / final-state properties

Typical properties of the fully cured material after the recommended cure schedule.

Property Value Unit Method / condition
Hardness 88 Shore D Cured material
Glass transition temperature (Tg) 77.0 °C Cured material
Dielectric strength 410 volts/mil Cured material
Volume resistivity 6.00×10¹³ ohm·cm @ 25°C
Lap shear strength, Al to Al 15 (2,200) N/mm² (psi) Sample cured 2 hr @ 65°C