LOCTITE ABLESTIK 2111

Harmonization Code : 8529.90 | Parts solely or principally used for TV, radio, and transmission

LOCTITE ABLESTIK 2111

Main features

  • Thixotropic Vertical/Overhead Bonding
  • 24 N/mm^2 Aluminum Lap Shear
  • Glass/Metal/Plastic Substrate Compatibility

Product Description

LOCTITE ABLESTIK 2111 BIPAX is a thixotropic, two-component epoxy adhesive formulated for ease of use, with a non-drip, non-sag rheology suited to vertical and overhead assembly work. Supplied as a hazy white resin and hardener at a 100:30 mix ratio in a BIPAX mixing-dispenser package, this solvent-free system cures at room temperature over 24 hours or faster with an accelerated schedule, and supports continuous service from -70°C to 100°C. It offers good wetting, improved impact strength, and excellent thermal, mechanical shock, and environmental resistance, making it suitable for bonding, laminating, staking, repair, and manufacturing across glass, ceramic, fabric, wood, leather, most metals, and many plastics.

Key features

  • Non-drip, non-sag rheology: Thixotropic formulation with good wetting for vertical and overhead applications.
  • High lap shear strength: 24 N/mm² (3,500 psi) on aluminum-to-aluminum bonds.
  • Broad substrate versatility: Bonds glass, ceramic, fabric, wood, leather, most metals, and many plastics.

Applications / Suitable for: Bonding, laminating, staking, repair, and manufacturing assembly applications across a wide range of substrates.

Product Family

ABLESTIK 2111

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Hazy White
Refractive index
1.53
Specific Gravity
1.24
Physical Properties
Viscosity
40000 mPa.s
Thermal Properties
Glass Transition Temperature (Tg)
45 °C
Operating Temperature
-70 to 100 °C
Electrical Properties
Volume Resistivity
9.500000000 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of the uncured, mixed material prior to cure.

Property Value Unit Method / condition
Mix ratio (Resin : Hardener) 100 : 30 by weight —
Viscosity, mixed 40,000 mPa·s (cP) @ 25°C, spindle TF, 10 rpm
Specific gravity, mixed 1.24 — Mixed material
Pot life 40 / 20 minutes @ 25 g mass / @ 100 g mass, mixed
Technical properties

After-processing / final-state properties

Typical properties of the fully cured material after the recommended cure schedule.

Property Value Unit Method / condition
Hardness 82 Shore D Cured material
Glass transition temperature (Tg), ultimate 45.0 °C Cured material
Elongation 26 % Cured material
Water absorption 3.3 % After 24 hours
Lap shear strength, Al to Al 24 (3,500) N/mm² (psi) Cured material