LOCTITE ABLESTIK 2106T

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE ABLESTIK 2106T

Main features

  • Shore D 72 within 60 Minutes
  • 410 V/mil Dielectric Strength
  • Metal-to-Masonry Multi-Substrate Bonding

Product Description

LOCTITE ABLESTIK 2106T BIPAX is a two-component, solvent-free epoxy adhesive designed for high-strength structural bonding applications. Supplied as a light yellow to orange liquid at a 110:93 resin-to-hardener mix ratio in a BIPAX mixing-dispenser package, it cures at room temperature in 4 to 6 hours or with an accelerated 1-hour cure at 65°C, developing significant handling strength within an hour of mixing. The adhesive is electrically insulating with low shrinkage and chemical resistance, and bonds a wide range of substrates including metals, phenolic plastics, polyester, glass, glass fabrics, ceramics, rubbers, and masonry materials. It supports continuous service from -60°C to 115°C, with intermittent exposure tolerance up to 150°C.

Key features

  • Fast property development: Reaches Shore D 72 hardness within 60 minutes of mixing at 25°C.
  • Electrically insulating: Volume resistivity of 5×10¹¹ ohm-cm at 25°C.
  • Broad substrate compatibility: Bonds metals, plastics, glass, ceramics, rubbers, and masonry materials.

Applications / Suitable for: High-strength structural assembly bonding across metals, plastics, glass, ceramics, and masonry/construction materials.

Product Family

ABLESTIK 2106T

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Light Yellow
Specific Gravity
1.22
Physical Properties
Viscosity
3600 mPa.s
Thermal Properties
Glass Transition Temperature (Tg)
25 °C
Operating Temperature
-60 to 115 °C
Electrical Properties
Volume Resistivity
500000000000 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of the uncured, mixed material prior to cure. Note the short pot life — use promptly after mixing.

Property Value Unit Method / condition
Mix ratio (Resin : Hardener) 110 : 93 by weight —
Viscosity, mixed 3,600 mPa·s (cP) @ 25°C
Specific gravity, mixed 1.22 — Mixed material
Pot life 5 minutes Mixed material; high exotherm, use immediately
Technical properties

After-processing / final-state properties

Typical properties of the fully cured material after the recommended cure schedule.

Property Value Unit Method / condition
Hardness, 60 minutes 72 Shore D @ 25°C, 60 min after mixing
Glass transition temperature (Tg) 25 °C Cured material
Volume resistivity 5×10¹¹ ohm·cm @ 25°C
Dielectric strength 410 volts/mil Cured material
Lap shear strength, Al to Al 1.37 (200) N/mm² (psi) Cured material