LOCTITE ABLESTIK 2101

Harmonization Code : 5906100000 | Adhesive tape of a width not exceeding 20cm

LOCTITE ABLESTIK 2101

Main features

  • 23 N/mm^2 Aluminum Lap Shear
  • High-Resistivity Electrical Insulation
  • Fuel, Oil, and Acid Resistance

Product Description

LOCTITE ABLESTIK 2101 BIPAX is a two-component, non-conductive epoxy adhesive supplied as a clear to slightly hazy liquid at a 100:25 resin-to-hardener mix ratio. Packaged in a convenient BIPAX mixing-dispenser for easy mixing, it cures at room temperature over 24 hours or faster with a heat cure of 4 hours at 65°C, and is suitable for continuous service from -60°C to 135°C. The adhesive bonds metals, ceramics, glass, wood, leather, and many rigid plastics, and is well suited to laminating, bonding, and repair applications requiring structural, mechanical, and electrical performance. Cured material offers strong electrical insulation and broad chemical resistance, including to petroleum solvents, fuels, and mild acids and alkalis.

Key features

  • High lap shear strength: 23 N/mm² (3,300 psi) on aluminum-to-aluminum bonds.
  • Good electrical insulator: Volume resistivity of 6×10¹⁵ ohm-cm at 25°C.
  • Easy mixing: Supplied in a BIPAX package for convenient, uniform two-component mixing.

Applications / Suitable for: Laminating, bonding, and repair of metals, ceramics, glass, wood, leather, and rigid plastics where structural, mechanical, and electrical insulating performance are required.

Product Family

ABLESTIK 2101

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Silver
Specific Gravity
1.2
Physical Properties
Viscosity
19000 mPa.s
Thermal Properties
Glass Transition Temperature (Tg)
62 °C
Operating Temperature
-60 TO 135 °C
Electrical Properties
Volume Resistivity
6000000000000000 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of the uncured, mixed material prior to cure.

Property Value Unit Method / condition
Mix ratio (Resin : Hardener) 100 : 25 by weight —
Viscosity, mixed 19,000 mPa·s (cP) @ 25°C
Specific gravity, mixed 1.2 — Mixed material
Pot life 30 minutes @ 25°C, mixed
Technical properties

After-processing / final-state properties

Typical properties of the fully cured material after the recommended cure schedule.

Property Value Unit Method / condition
Glass transition temperature (Tg) 62.0 °C Cured material
Volume resistivity 6×10¹⁵ ohm·cm @ 25°C
Dielectric strength 370 volts/mil Cured material
Coefficient of linear thermal expansion 55 ppm/°C Cured material
Lap shear strength, Al to Al 23 (3,300)